说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 高碳高铬蓖条
1)  High Carbon-High Chromium Steel Strip
高碳高铬蓖条
2)  High-carbon ferrochrome
高碳铬铁
1.
It analyzed interrelations among the carbon, silicon and sulphur in high-carbon ferrochrome, slag basicity and furnace temperature, coke's sulphur influenced on desulphurization are also discussed, many effective measures are taked for lessening sulphur content in high-carbon ferrochrome.
文章从理论上分析了高碳铬铁合金中碳、硅、硫含量的相互关系,炉渣碱度对合金含量的影响,提高炉温对 炉渣脱硫的作用以及焦炭含硫量的影响等。
3)  high carbon ferrochrome
高碳铬铁
1.
It analyses the changeable TiO_2 content in chrome ore and the structural form,the balance of Ti,the reaction mechanism of Ti and its existence form in alloys,the affect factor of Ti content in alloys,and benefits and control methods during the process of smelting low titanium high carbon ferrochrome.
分析了低钛高碳铬铁生产过程中铬矿TiO_2含量变化与结构形式,冶炼过程中Ti的平衡、反应机理和在合金中的存在形式,合金含Ti量高低的影响因素,以及效益与控制方法。
2.
It introduces technological condition and result of smelting high carbon ferrochrome with Xinjiang's high melting point and low grade chromes.
介绍了使用新疆高熔点、低品位铬矿冶炼高碳铬铁的工艺条件和结果,实践证踢通过合理地控制操作,可以得到较理想的技术经济指标。
3.
Based on the principle and characteristics of medium frequency furnace, analysis on physical and chemical performance of liner material , better technological economic indexes and benefits of adaptation to 2 tons medium frequemcy furnace for resmelting high carbon ferrochrome are realizde by pilot production and industrialized production.
采用2 t中频炉重熔高碳铬铁,根据中频炉的原理及特点,对炉衬材料的物化性能进行了分析,通过试生产和工业化生产,取得了较好的技术经济指标和经济效益。
4)  High C Cr Steel
高碳铬钢
5)  high carbide high chromium steel
高碳高铬钢
1.
The chemical compositions of high carbide high chromium steel and chromium-bearing grey cast iron were optimized through orthogonally designed experiments which were carried out on a horizontal cantilevered centrifugal machine to compound the steel and cast iron by way of a centrifugal casting process.
通过正交设计实验优化得到了高碳高铬钢、含铬灰铸铁的最优成分;采用卧式悬臂离心实验机对高碳高铬钢/含铬灰铸铁进行离心复合·在复合成功的基础上,利用金相显微镜对不同实验条件下的复合界面进行了对比、分析·结果表明:经离心复合铸造,高碳高铬钢/含铬灰铸铁复合界面为结合紧密的复合层;复合试样经1080℃保温1h,水淬+500℃回火1h处理后,复合界面碳化物扩散更充分,但对复合界面宽度没有影响;浇注温度提高,复合界面宽度增加,当高碳高铬钢液浇注温度由1460℃提高到1480℃时,复合界面宽度增加了100μm
6)  high C-Cr cast steel
高碳铬铸钢
1.
Results show that RE and heat, treatment improves the morphology and the distribution of carbide and increases the impact toughness of high C-Cr cast steel.
研究了稀土与热处理对高碳铬铸钢碳化物的形态及冲击韧性的影响。