1) sulfate-modified titanium-bearing blast furnace slag
硫酸盐掺杂的含钛高炉渣
1.
Using calcined sulfate-modified titanium-bearing blast furnace slag(STBBFS) as photocatalyst,the photocatalytic activity of STBBFS photocatalyst toward a Cr(VI)-citric acid [Cr(VI)-CA] system and a Cr(VI)-citric acid-ferric nitrate [Cr(VI)-CA-FN] system was studied.
采用煅烧的硫酸盐掺杂的含钛高炉渣(sulfate-modified titanium-bearing blast furnace slag,STBBFS)作为光催化剂,研究了Cr(VI)-柠檬酸[Cr(VI)-CA]复合体系和Cr(VI)-柠檬酸-硝酸铁[Cr(VI)-CA-FN]复合体系对STBBFS催化剂光催化活性的影响。
2.
Using calcined sulfate-modified titanium-bearing blast furnace slag as photocatalyst, the photocatalytic reduction of Cr(VI) in Cr(VI)-acetic acid (AA) compound system was studied.
采用煅烧的硫酸盐掺杂的含钛高炉渣作光催化剂,研究了Cr(VI)-乙酸(AA)复合体系中Cr(VI)的光催化还原效率,考察了初始pH值、Cr(VI)初始浓度、AA/Cr(VI)体积比、协同效率因子、光催化剂使用寿命等因素的影响。
2) sulfuric acid-modified titanium-bearing blast furnace slag
硫酸掺杂的含钛高炉渣
1.
Perovskite type sulfuric acid-modified titanium-bearing blast furnace slag(STBBFS) photocatalysts were prepared by the high energy ball milling method at 400℃ for 2h.
采用高能球磨法,添加不同比例硫酸,在400℃煅烧2h合成了具有钙钛矿型的硫酸掺杂的含钛高炉渣催化剂(sulfuric acid-modified titanium-bearingblast furnace slag,STBBFS)。
3) Vanadium oxide modified titanium-bearing blast furnace slag
钒掺杂的含钛高炉渣
4) titanium-bearing blast furnace slag
含钛高炉渣
1.
Development of study on comprehensive utilization of titanium-bearing blast furnace slag;
含钛高炉渣综合利用研究的进展
2.
Synthesis of (Ca, Mg) α′-Sialon-AlN-TiN powders from titanium-bearing blast furnace slag;
含钛高炉渣合成(Ca,Mg)α′-Sialon-AlN-TiN粉末
3.
Preliminary study of synthesis compound fertilizer from titanium-bearing blast furnace slag
由含钛高炉渣合成复合肥初探
5) Ti-bearing blast furnace slag
含钛高炉渣
1.
Green separation technique of Ti component from Ti-bearing blast furnace slag;
含钛高炉渣中钛组分的绿色分离技术
2.
The significance and present research state of comprehensively utilizing Ti-bearing blast furnace slag are overviewed.
对含钛高炉渣综合利用意义、研究现状进行了概述,分析了含钛高炉渣利用过程中存在的主要问题。
3.
Modifying the phase structure of Ti-bearing blast furnace slag by using physical chemistry method is the key to utilization of Ti-bearing blast furnace slag;Back scattered image,X-ray energy spectrum analysis and X-ray diffraction analysis of the raw slag and modified slag were carried out.
改变含钛高炉渣中矿相组成的研究是含钛高炉渣综合利用的关键;通过背散射电子形貌像、X射线能谱分析和X射线物相分析等手段,对氧化前的含钛高炉渣及其氧化改性后的渣样进行分析,表明氧化后渣中含钛相的形貌、成分和相结构等发生变化;钛的赋存状态也发生相应的改变。
补充资料:羟胺硫酸盐、硫酸羟胺、硫酸胲
CAS : 10039-54-0
分子式: H8N2O6S
分子量: 164.14
熔点: 170℃
中文名称: 羟胺硫酸盐、硫酸羟胺、硫酸胲
英文名称: Hydroxylamine sulfate、Hydroxylamine, sulfate(2:1) (salt)、hydroxylamine, sulfate (2:1)、bis(hydroxylamine) sulfate、hydroxylamine neutral sulfate、hydroxylamine, sulfate、hydroxylamine, sulfate (2:1) (salt)、oxammonium sulfate、Hydroxylamine,sulfate(2:1)(salt)
性质描述: 无色或白色结晶。熔点约170℃(分解),沸点56.5℃,密度1.204g/cm3。溶于冷水、乙醇和甲醇。极易吸湿。羟胺性质很不稳定,在常温下逐渐分解,在较高温度下会爆炸,故通常将其制成比较稳定的硫酸盐和盐酸盐。其中以硫酸羟胺为最常用。
生产方法:
1.以甲乙酮和硫酸及氨反应,生成甲乙酮肟,然后与硫酸反应,经水解制得硫酸羟胺(结晶型)和甲乙酮和硫铵副产。
2.由亚硝酸钠和亚硫酸氢铵混合进行反应,于低温下通入二氧化硫使反应物吸收得羟胺二磺酸盐,再进行水解,制得硫酸羟胺。3.采用硫酸与硝基烃反应亦可制得硫酸羟胺。
用途: 用作还原剂、显影剂和橡胶硫化剂。该品是合成已内酰胺的重要原料。也是医药、农药的中间体,用于生产一系列异噁唑衍生物、磺胺药物和维生素B6、B12。衍生物肟或羟肟酸衍生物可用来生产农药杀虫剂、杀菌剂和除草剂。还可用于高分子合成原料和化合物的精制、聚合催化剂及化学分析试剂等。
分子式: H8N2O6S
分子量: 164.14
熔点: 170℃
中文名称: 羟胺硫酸盐、硫酸羟胺、硫酸胲
英文名称: Hydroxylamine sulfate、Hydroxylamine, sulfate(2:1) (salt)、hydroxylamine, sulfate (2:1)、bis(hydroxylamine) sulfate、hydroxylamine neutral sulfate、hydroxylamine, sulfate、hydroxylamine, sulfate (2:1) (salt)、oxammonium sulfate、Hydroxylamine,sulfate(2:1)(salt)
性质描述: 无色或白色结晶。熔点约170℃(分解),沸点56.5℃,密度1.204g/cm3。溶于冷水、乙醇和甲醇。极易吸湿。羟胺性质很不稳定,在常温下逐渐分解,在较高温度下会爆炸,故通常将其制成比较稳定的硫酸盐和盐酸盐。其中以硫酸羟胺为最常用。
生产方法:
1.以甲乙酮和硫酸及氨反应,生成甲乙酮肟,然后与硫酸反应,经水解制得硫酸羟胺(结晶型)和甲乙酮和硫铵副产。
2.由亚硝酸钠和亚硫酸氢铵混合进行反应,于低温下通入二氧化硫使反应物吸收得羟胺二磺酸盐,再进行水解,制得硫酸羟胺。3.采用硫酸与硝基烃反应亦可制得硫酸羟胺。
用途: 用作还原剂、显影剂和橡胶硫化剂。该品是合成已内酰胺的重要原料。也是医药、农药的中间体,用于生产一系列异噁唑衍生物、磺胺药物和维生素B6、B12。衍生物肟或羟肟酸衍生物可用来生产农药杀虫剂、杀菌剂和除草剂。还可用于高分子合成原料和化合物的精制、聚合催化剂及化学分析试剂等。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条