2) hot corrosion
热腐蚀
1.
Effects of sputtered TiAlCr coatings on hot corrosion resistance of TiAl intermetallics in molten sulphate;
TiAlCr涂层对TiAl金属间化合物抗熔融硫酸盐热腐蚀的影响
2.
Oxidation and hot corrosion behavior of a composite MCrAlY/enamel coating;
MCrAlY/搪瓷复合涂层的抗高温氧化及热腐蚀性能
3.
Structure and high temperature hot corrosion of palladium modified aluminide coatings on nickel-base superalloy;
钯改性镍基高温合金铝化物涂层的组织和热腐蚀性能
3) hot salt corrosion
热盐腐蚀
5) hydrothermal etching
水热腐蚀
1.
A novel silicon-based micron/nanometer structural composite system, silicon nanoporous pillar array(Si-NPA), was prepared on the substrate of single-crystal silicon (sc-Si) wafers by a hydrothermal etching method; and the studies on its morphological structural and optical properties were carried out.
采用水热腐蚀技术在单晶硅衬底上制备出一种新的硅微米 /纳米结构复合体系——硅纳米孔柱阵列 (Si -NPA) ,并对其表面形貌、结构及光学特性进行研究 。
6) High heat
高热腐蚀
补充资料:腐蚀热力学
分子式:
CAS号:
性质:阐述金属发生腐蚀的根本原因,介绍判断腐蚀倾向的理论。从热力学观点看,腐蚀过程是由于金属与其周围介质构成了一个热力学上不稳定的体系,此体系有从不稳定趋向稳定的倾向。对于各种金属来说,这种倾向极不相等。它的大小可通过腐蚀反应的自由能变化(△G)T,P来衡量,若(△G)T,p<0,则腐蚀反应可能发生,但它不能说明腐蚀的速度问题。
CAS号:
性质:阐述金属发生腐蚀的根本原因,介绍判断腐蚀倾向的理论。从热力学观点看,腐蚀过程是由于金属与其周围介质构成了一个热力学上不稳定的体系,此体系有从不稳定趋向稳定的倾向。对于各种金属来说,这种倾向极不相等。它的大小可通过腐蚀反应的自由能变化(△G)T,P来衡量,若(△G)T,p<0,则腐蚀反应可能发生,但它不能说明腐蚀的速度问题。