1) primary Al_3Fe phase
初生Al3Fe相
1.
The effect of Mg on the morphology of primary Al_3Fe phase in hypereutectic Al-10%Fe casting alloy was investigated.
研究了Mg元素对铸造Al-10%Fe过共晶合金初生Al3Fe相形态的影响。
2.
The influence of thermal rate treatment on the mechanical property of Al-5%Fe alloy and the morphology of primary Al_3Fe phase was studied.
研究了热速处理工艺对Al 5%Fe合金力学性能和初生Al3Fe相形貌的影响。
2) primary Al_3Fe
初生Al3Fe
1.
The melt treatment by mixing high temperature melt with low temperature melt was adopted to refine the primary Al_3Fe compound.
为细化Al-5%Fe合金中的初生Al3Fe相,研究了高、低温熔体混合工艺对合金组织的影响。
3) Al_3Fe phase
Al3Fe相
1.
The effect of alloying elements manganese,copper,titanium and boron on the morphology and distribution of the primary Al_3Fe phase in Al-10%Fe alloys was studied.
研究了Mn、Cu、Ti、B等合金元素对Al-10%Fe合金初生Al3Fe相大小、形貌及分布的影响。
2.
The results show that there exists more thick needle-plate like and needle like Al_3Fe phase without superheating and chilling; adding Al-Fe alloy at 1000℃, the microstructure is composed of small needle like iron-rich phases,however, the microstructure becomes coarser when the temperature is too high; the microstructure becomes thinner and thinner with the rise of temper.
研究了在高温过热Al-5%Fe合金熔体中分别加入Al锭和同种成分的Al-Fe合金两种热速处理工艺对Al3Fe相形貌的影响。
4) Al3Fe morphology
Al3Fe相形貌
1.
The characteristics of Al3Fe morphology change and the hardness of Al-Fe alloy with various Fe contents were investigated.
研究了不同含Fe量的Al Fe合金中Al3Fe相形貌和Al Fe合金硬度的变化特点。
5) Al 3Fe
Al3Fe
6) Primary Phase
初生相
1.
Evolution of Primary Phase in A357 Semi-solid Aluminum Alloy During Reheating and Forming Process;
A357半固态初生相在二次加热和成形过程中的演变行为
2.
Correlation between crystallization kinetics of amorphous alloys and primary phases during crystallization;
非晶合金的晶化动力学与初生相的内在联系
3.
Influence of RE Element Y on Morphology of Primary Phase in A356 Aluminum Alloy;
Y对A356铝合金半固态初生相形貌的影响