1) morphology of primary phase
初生相形貌
1.
The results indicate that the morphology of primary phase in semi-solid A356 prepared by compound process is char.
利用复合工艺制备了A356铝合金半固态浆料,研究了半固态A356铝合金初生相形貌的分形特征。
2.
The semi-solid slurry of A356 alloy is prepared by lowsuperheat pouring, and the transform of morphology of primary phase in semi-solid A356 alloy during isothermal holding in solidliquid phase region is studied The effects of holding temperature and holding time on the morphology of primary phase in semisolid A356 alloy are investigated.
利用低过热度浇注工艺制备了A356-Sc铝合金半固态浆料,研究了A356-Sc铝合金半固态初生相形貌在固液相区等温保温中的转变,讨论了等温温度和保温时间对A356-Sc铝合金半固态初生相形貌演变的影响。
3) phase morphology
相形貌
1.
Study on phase morphology and mechanical properties of epoxy system toughened by fluorinated poly(ether ether ketone);
含氟聚醚醚酮增韧环氧树脂相形貌与性能研究
2.
Now, phase morphology of alloy can be changed by chemical modification, superheating treatment and electromagnetic vibration.
研究了超声处理对Mg-9Al合金Mg17Al12相形貌的影响。
4) morphology of Al4C3 phase
Al4C3相形貌
5) Al3Fe morphology
Al3Fe相形貌
1.
The characteristics of Al3Fe morphology change and the hardness of Al-Fe alloy with various Fe contents were investigated.
研究了不同含Fe量的Al Fe合金中Al3Fe相形貌和Al Fe合金硬度的变化特点。