1) deep drawing steel
深冲钢
1.
It is analyzed the controlling-sulfur technique in smelting of SPHD deep drawing steel.
对唐山建龙实业有限公司SPHD深冲钢冶炼过程中的控硫技术进行了分析。
2.
This paper according to the concrete application on Cold rolling deep drawing steel mechanical property optimization, introduces the idea of six sigma administration and main analytical method of DMAIC each phase.
本文根据六西格玛管理在冷轧深冲钢机能优化中应用的实际情况,介绍了六西格玛管理的技术方法和项目运作在DMAIC各阶段的主要分析方法。
2) deep drawing steel sheet
深冲钢板
1.
Texture and modeling calculation of r values of deep drawing steel sheet;
深冲钢板的织构及塑性应变比r值的模型计算
2.
Recrystallization and formation of {111} texture in micro-carbon deep drawing steel sheet
微碳深冲钢板的再结晶与{111}织构的形成过程
3.
Influence of dissolved carbon content on recrystallization γ-fibre texture in ultra-low carbon deep drawing steel sheet with high purity was investigated and the relationships between dissolved carbons and recrystallization γ-fibre texture and {111} <112> and {111} < 110 > textures were analysed by 3-dimensional orientation distribution function.
借助三维取向分布函数探讨了高纯超低碳深冲钢板的固溶碳含量对再结晶γ织构的影响,分析了固溶碳与再结晶γ织构及其中的{111}<112>和{111}<110>织构之间的关
3) IF deep drawing steel sheet
IF深冲钢板
4) IF deep-drawing steel
IF深冲钢
5) deep-drawing steel sheet
深冲IF钢板
1.
Estimation of plastic strain ratio-R-value is essential to accomplish the on-line control of property and quality of deep-drawing steel sheet.
采用最大熵三维取向分布函数(MEMODF)和简ODF法,按照织构多晶体连续力学法(CMTP法),遵循Konchend(?)rfer模型,选择非二次型屈服函数来预估多晶体(深冲IF钢板)的塑性应变比R值。
6) extra-deep drawing IF steel
超深冲IF钢
1.
The recrystal course is observed through annealing temperature of 800℃ and variation annealing time in extra-deep drawing IF steel.
本文选用了超深冲IF钢,经1200℃开轧、930℃终轧、700℃卷取和80%冷轧后,在800℃不同时间退火并观察其再结晶过程。
补充资料:深冲钢deep
drawingsteel:适合于深冲加工方法制造制件用的薄钢板或钢带。