说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> Fe78Si9B13非晶合金
1)  amorphous Fe78Si9B13 alloy
Fe78Si9B13非晶合金
1.
The plastic deformation property of amorphous Fe78Si9B13 alloy was investigated by tension and gas pressure bulging at elevated temperature.
通过高温拉伸及胀形实验,研究了Fe78Si9B13非晶合金的塑性变形性能。
2)  amorphous Fe_(78)Si_9B_(13) alloy
非晶Fe78Si9B13合金
1.
The amorphous Fe_(78)Si_9B_(13) alloy was partially crystallized when it was irradiated by CO_2 laser beam with 20mm spot diameter for 20 sec at 250W and 300W as the laser power.
在CO2激光散光斑直径20mm的情况下,分别选择在不同功率静置的条件下辐照Fe78Si9B13非晶带实现部分晶化·用穆斯堡尔谱、X射线衍射和扫描电镜对原始非晶样品(Fe78Si9B13)和晶化后样品的微观结构进行了分析·结果表明:在CO2激光散光斑直径一定的条件下(20mm),分别选择激光功率250W和300W辐照非晶Fe78Si9B13样品20s,非晶样品可以实现约6%和9%的晶化·激光辐照非晶Fe78Si9B13合金的晶化相为αFe(Si),样品发生了织构现象,晶粒沿(200)面大量析出·激光晶化相产生在非晶带表面晶化层中·在其他条件一定的情况下,样品的晶化量随着激光功率的增加而增加
3)  Fe78Si9B13 amorphous alloy ribbons
Fe78Si9B13非晶薄带
1.
The Fe78Si9B13 amorphous alloy ribbons with the thickness of 25 μm and the width of 4.
5mm、厚25μm的Fe78Si9B13非晶薄带,并用Q800动态热机械分析仪(DMA)测试了非晶薄带的弹性模量、线形变和线膨胀系数,并分析了它们随着退火工艺及测试温度的变化关系。
2.
In this paper, Fe78Si9B13 amorphous alloy ribbons with 25 μm thickness and 4.
5mm、厚25μm的Fe78Si9B13非晶薄带。
3.
In this paper,the influences of frequency and magnetic field intensity on the magnetic induction effect and the impact factor for the changing magnitude of magnetic induction effect of Fe78Si9B13 amorphous alloy ribbons were studied.
研究了频率、磁场强度对Fe78Si9B13非晶薄带的磁感应效应及影响磁感应效应变化幅度的因素。
4)  amorphous alloy
非晶合金
1.
Current study and advances on superplastic forming of bulk amorphous alloy;
大块非晶合金超塑性变形的研究现状与发展
2.
Influence of Oxidation on the Accuracy of DSC and TG Measurements for Amorphous Alloys;
试验条件对非晶合金DSC与TG测量的影响
3.
Study of behavior of non-isothermal crystallization of amorphous alloy Mg_(65)Cu_(22)Ni_3Y_(10);
Mg_(65)Cu_(22)Ni_3Y_(10)非晶合金的非等温晶化行为研究
5)  amorphous alloys
非晶合金
1.
Correlation between crystallization kinetics of amorphous alloys and primary phases during crystallization;
非晶合金的晶化动力学与初生相的内在联系
2.
Crystallization kinetics of Ni_(59)Zr_(16)Ti_(13)Si_3Sn_2Nb_7 amorphous alloys;
Ni_(59)Zr_(16)Ti_(13)Si_3Sn_2Nb_7非晶合金的晶化动力学
3.
5 amorphous alloys were prepared by a single roller melt-spinning technique in an air atmosphere.
5非晶合金的非等温晶化的动力学行为。
6)  metallic glass
非晶合金
1.
Plastic deformation of bulk metallic glass (BMG) Zr55Al10Ni5Cu30 was investigated by nanoindentation experiments at room temperature.
对Zr55Al10Ni5Cu30块状非晶合金进行了室温纳米压痕实验,利用扫描电子显微镜、透射电子显微镜揭示了非晶合金的微区形变特征。
2.
The deformation and fracture behavior under quasi-static compressive loading of a bulk metallic glass,Zr-Ti-Ni-Cu,was studied using instron universal-testing machine(IUTM) and scanning electron microscopy(SEM) at room temperature.
利用IUTM和SEM研究了Zr-Ti-Ni-Cu块状非晶合金的准静态单轴压缩变形和断裂行为。
3.
5 metallic glass has been studied by DSC and XRD.
5块状非晶合金的相变动力学。
补充资料:Dithane z-78

国标编号 ----
CAS号 12122-67-7
分子式 C4H6N2S4Zn;(CH2NHCSS)2Zn
分子量 275.75

灰白色粉末,工业品为淡黄色粉末,略带臭鸡蛋味,吸湿性强;蒸汽压 <10-4mPa闪点>100℃;熔点;溶解性:不溶于水,不溶于多数有机溶剂;密度:1.74;稳定性:稳定;危险标记 ;主要用途:用作硫化促进剂、农用杀菌剂,有65%及80%可湿性粉剂

2.对环境的影响
一、健康危害

侵入途径:吸入、食入。
健康危害:中毒主要影响中枢神经系统,对肝、肾有一定的损害。对皮肤和粘膜有刺激作用,可引起皮肤过敏。长期接触可能有引起甲状腺肿作用。

二、毒理学资料及环境行为

急性毒性:LD50>5200mg/kg(大鼠经口);LC501850mg/m3(大鼠吸入);人经口5~g/kg(估计量)致死
其降解产物乙撑硫脲可引起试验鼠甲状腺肿大。

代森锌是有机硫杀菌剂,属低毒性。在1987~1988年,我们对不同厂家的制剂,在贮存过程中降解生成乙撑硫脲的变化,进行研究。结果表明,4种样品经16个月贮存,不论在开口或封口条件下,乙撑硫脲含量均随时间延长而增加。在贮存1个月后,乙撑硫脲含量就达到或超过允许标准。此外,乙撑硫脲不但易被植物吸收,输送到植物各部位,而且在土壤中淋溶程度也大。乙撑硫脲是一种潜在致甲状腺肿、致畸、致突变和在高剂量下致癌的化合物。

危险特性:遇明火、高热可燃。受热分解,放出氮、硫的氧化物等毒性气体。
燃烧(分解)产物:一氧化碳、二氧化碳、氮氧化物、硫化物、氧化锌。

3.现场应急监测方法
 

4.实验室监测方法
气相色谱法(蘑菇罐头)《农药残留量气相色谱法》国家商检局编

5.环境标准
前苏联(1976) 职业环境空气中最高容许浓度 0.5mg/m3(气溶胶)
前苏联(1978) 环境空气中最高容许浓度 0.01mg/m3(一次值)
0.006mg/m3(日均值)
前苏联(1978) 生活饮用水和娱乐用水水体中有害物质的最大允许浓度 0.03mg/L

6.应急处理处置方法

一、泄漏应急处理

 切断火源。戴好防毒面具和手套。避免扬尘,小心扫起,置于袋中转移至安全场所。如大量泄漏,收集回收或载害处理后废弃。

二、防护措施

呼吸系统防护:高浓度环境中,建议佩戴供气式呼吸器。
眼睛防护:可采用安全面罩。
防护服:穿工作服。
手防护:必要时戴防护手套。
其它:注意个人清洁卫生。

三、急救措施

皮肤接触:脱去污染的衣着,用大量流动清水彻底冲洗。
眼睛接触:立即翻开上下眼睑,用流动清水或生理盐水冲洗。就医。
吸入:迅速脱离现场至空气新鲜处。保持呼吸道通畅。呼吸困难时给输氧。呼吸停止时,立即进行人工呼吸。就医。
食入:误服者给饮足量温水,催吐,就医。

灭火方法:泡沫、二氧化碳、干粉、砂土。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条