1) Ca-CaCl2 molten salt method
Ca-CaCl2熔盐法
1.
In this paper,the extra-low-oxygen yttrium metal is prepared by Ca-CaCl2 molten salt method.
主要开展了用Ca-CaCl2熔盐法制备低氧金属钇(Y)的研究。
2) CaCl_2-NaCl molten salt
CaCl2-NaCl熔盐
1.
The mechanism of ZrO_2 direct electrodeoxidation into Zr in CaCl_2-NaCl molten salt was studied by Cyclic Voltammetry and Chronoamperometry in the temperature range of 800~860℃.
采用循环伏安法和记时电流法研究800~860℃下ZrO2电极在CaCl2-NaCl熔盐中还原过程的反应机理。
3) molten CaCl_2
CaCl2熔盐
4) Ca-CaCl_2 fused-salt method
Ca-CaCl_2熔盐法
1.
In this paper, the research that the extra-low-oxygen rare-earth metal Yttrium is prepared by Ca-CaCl_2 fused-salt method and electrochemistry purification method is mainly developed.
本文主要开展了用Ca-CaCl_2熔盐法和电化学提纯法制备高纯低氧稀土金属钇(Y)的研究。
5) CaCl2 method
CaCl2法
6) calcium chloride-tolerance
耐CaCl2盐
补充资料:熔盐电解制粉法
熔盐电解制粉法
preparation of powder by electrolysis from fused salt
rongyan dlanj一e zhlfenfo熔盐电解制粉法(preparation of powder byeleetrolysis from fused salt)高温下电解金属的熔盐制取金属粉末的一种粉末制取方法。 熔盐电解和水溶液电解的基本原理一致。有些金属如钠等活泼元素,只能由电解其熔盐如氯化钠来制取。而电解氯化钠水溶液只能得到氢氧化钠和氯气、氢气,得不到金属钠。此外,难熔金属错、社、敏、担和妮等对氧的亲和力大,不会从水溶液中析出,也只能用熔盐电解法制取。熔盐电解中的电解质是用欲电解制取的金属的熔点较低的卤化物、氧化物以及氟担酸盐、氟氧妮酸盐等。 熔盐电解法可以制取各种单一金属,也可以制取合金,还可以制备硼化物、硅化物等。熔盐电解法的缺点是:阴极上生成的松散淀积物难以从电解槽中取出(低熔点的铿、钠、钙、镁和铝等除外)且在阳极上有氟气、氯气体析出,污染环境。 以熔盐电解制取担粉为例,其工艺为:电解质使用KZTaF:+KCI十KF的混合熔盐,电解温度为75oC,将Ta20。定时加到电解质中,在熔融电解质中熔解,作为钮的来源。电解时所用柑竭由铁或石墨制成,置于电炉中加热,并作阳极;阴极用铝棒制成,置于钳涡中央。电解时,金属担在钥阴极棒上淀积成“梨状物”,周期地取出,换上新的钥阴极棒。“梨状物”冷却后,经破碎、研磨之后,洗去粘附的电解质,干燥。所得钮粉的纯度可达99.8%~99.9%,比金属热还原法制取的担粉纯度高。 采用类似工艺也可以制取妮粉,错粉、社粉和被粉等。 (张智伯)