1)  7A04 super-high strength aluminum alloy
7A04超硬铝合金
2)  7A04 ultra-high strength aluminum alloys
7A04超高强铝合金
3)  7A04 aluminum alloy
7A04铝合金
1.
Corrosion behavior of 7A04 aluminum alloy deposited with sodium chloride in simulated environment
表面沉积氯化钠的7A04铝合金在模拟环境中的腐蚀行为
2.
The effects of solid solution and recrystalization treatment on the microstructure and mechanical properties of 7A04 aluminum alloy by superplastic pre-treatment(SPPT) were investigated by means of optical microscope,mechanical tensile test and EDAX analysis.
采用力学性能检测、金相组织观察和能谱分析,试验研究了超塑预处理(SPPT)中固溶再结晶工艺对7A04铝合金组织和力学性能的影响。
3.
The effects of thermomechanical treatment on the structures and properties of 7A04 aluminum alloy were studied by mechanical tensile test,metallographic and TEM analysis.
研究了形变热处理工艺对7A04铝合金的组织和性能的影响。
4)  7A04 aluminium alloy
7A04铝合金
1.
Experimental research and strength prediction on aged strengthening of 7A04 aluminium alloy
7A04铝合金时效强化的试验研究及其强度计算
2.
Electrochemical performance of initial corrosion of 7A04 aluminium alloy in marine atmosphere
7A04铝合金在海洋大气环境中初期腐蚀的电化学特性
5)  superhard aluminium alloy
超硬铝合金
6)  7A04 alloy
7A04合金
1.
Microstructure evolution of 7A04 alloy in semi-solid state thixoforging;
7A04合金半固态触变模锻的组织演化
2.
Two kinds of different 7A04 alloys were used as experimental billets.
以两种状态的7A04合金为例,简要分析了二次加热工艺参数、模具预热温度等工艺参数对半固态模锻成形的影响,并重点研究了半固态模锻前后的显微组织变化及不同加热温度下的力学性能。
3.
The average grains size of 7A04 alloy by SPPT is Hum, however that by conventional treatment(CT) is 30μm.
采用超塑预处理工艺可使7A04合金晶粒细化到11μm,而传统处理工艺的晶粒为30μm。
补充资料:[3-(aminosulfonyl)-4-chloro-N-(2.3-dihydro-2-methyl-1H-indol-1-yl)benzamide]
分子式:C16H16ClN3O3S
分子量:365.5
CAS号:26807-65-8

性质:暂无

制备方法:暂无

用途:用于轻、中度原发性高血压。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条