1) free cold forging
自由冷镦
1.
Base on the method of numerical simulation,both free cold forging and opened cold forging of shaft with boss were analyzed.
基于数值模拟的方法,分析了凸台轴的自由冷镦和开式冷镦两种加工方法。
2) free compression
自由镦粗
1.
The computing formula of the two technology data,that is the technology deforming data “n” and every deforming degree “ε hn ”,can be deduced from the basic definition formula of the free compression deforming degree,its application method is mentioned.
从自由镦粗变形程度基本定义式 ,推导出了自由镦粗成形工艺的顶镦变形次数n和各次变形程度εhn,这两个自由镦粗变形基本工艺参数的设计计算公式 ,并举例说明了其应用方
3) automatic cold header
自动冷镦机
1.
Analysis of process of crankshaft of bolt combined automatic cold header in the lathe;
车床加工螺栓联合自动冷镦机曲轴工艺浅析
4) cold heading
冷镦
1.
Research on ductile fracture criteria and the application in cold heading process;
韧性断裂准则的研究及其在冷镦成形过程中的应用
2.
To introduce trial production course of ML08Al wire rod for cold heading from 150 mm×150 mm continuous casting billet.
介绍采用150 mm×150 mm连铸坯试制ML08A l冷镦线材的过程,从化学成分、低倍组织、高倍组织、力学性能等方面分析线材性能。
3.
Adopting the method of combining the Oyane Ductile Fracture Criteria with Finite Element Analysis(FEA) to analyze the deformation course of inner hexagonal bolt with 35K steel,the position for hexagonal bolt head to be easy broken and the cause are discussed,the crazing situations of inner hexagonal bolt in cold heading are forecasted,the results accord with practical breaking situation.
采用Oyane韧性断裂准则与有限元分析相结合的方法,对以35K为材料的内六角螺钉的成形过程进行分析,探讨内六角螺钉头易于开裂的部位及其原因,预测内六角螺钉冷镦过程中的开裂情况,结果与实际开裂情况相符合。
5) cold upsetting
冷镦
1.
Design method for improving cold upsetting mould service life by lining technology;
利用镶套技术提高冷镦模具寿命的设计方法
2.
On the basis of the analysis of the difficulties for forming the eccentric shaft by cold upsetting, the measures for solving the problem of material flow instability and the improvements in the structure of the die were proposed.
在分析了偏心轴冷镦工艺成形难点的基础上 ,提出了解决材料流动失稳的措施和对模具结构的改
3.
The design of cold upsetting process is usually carried out by an experienced designer from his own expertise, existing designs and the process rules.
冷镦工序设计通常由经验丰富的工艺人员根据已有的设计、工艺原则及其经验进行。
6) Cold-heading
冷镦
1.
Quality improvement of low carbon cold-heading wire for screw nut;
低碳冷镦螺母用线材的质量改进
2.
This paper introduced a green process method of miniature electrical machinery axle,which breaked through the traditional process method: it changes the turning both ends half a ball face for cold-heading,and becomes the outer circle to grinding to cold-drawing.
介绍了一种微型电机轴的绿色加工方法,它突破了微型电机轴传统的加工方法,改车削两端半球面为冷镦,变外圆磨削为冷拉。
3.
In this paper the chemical composition, strength and ductility of the steel were investigated according to the crack phenomenon in the 45# cold-heading wire cord steel.
本论文根据45#钢盘条加工过程中冷镦开裂的现象,对钢化学成分,及强度、塑性特性进行了分析研究。
补充资料:自动冷镦机、多工位螺栓自动冷镦机
| |||||||
主要参数内容 | 国际先进 | 国内先进 | 国内一般 | 国内落后 | 评定方法及说明 | ||
(一)加工精度 | 参照GB9166-88、JB/T3053-91 | ||||||
1、冲头夹持器模孔中心线对夹持器后支承面的垂直度(mm) 在100长度上 | 0.008 | 0.01 | 0.015 | >0.015 | |||
2、凹模座模孔中心线对凹模后座支承面的垂直度(mm) 在100长度上 | 0.008 | 0.01 | 0.015 | >0.015 | |||
3、冲头夹持器模孔中心线对滑块行程的平行度(mm) 在100行程上 | 0.016 | 0.02 | 0.02 | >0.02 | |||
4、滑块行程对机身上与凹模座贴合的垂直面的垂直度(mm) 在100行程上 | 0.016 | 0.02 | 0.02 | >0.02 | |||
5、工件头部对工件杆部中心线的偏移量(mm) | <0.20 | 0.20~0.25 | 0.25~0.30 | >0.30 | |||
(二)生产率(件/分) | |||||||
20mm | >80 | 70 | 65 | <65 | |||
30mm | >60 | 50 | 45 | <45 |