1) Ba-bearing aluminoferriate cement
含钡铁铝酸盐水泥
1.
The effect of gypsum content on the hydration,compressive strength and setting time of Ba-bearing aluminoferriate cement was presented.
介绍了石膏含量对含钡铁铝酸盐水泥的水化、抗压强度和凝结时间等性能的影响。
2) sulphoaluminate cement clinker containing barium
含钡硫铝酸盐水泥熟料
1.
Sintering sulphoaluminate cement clinker containing barium from low-grade barytes and studying on its properties;
利用低品位重晶石烧制含钡硫铝酸盐水泥熟料及其性能研究
3) barium containing sulphoaluminate cement
含钡硫铝酸盐水泥
1.
The minerals of the barium containing sulphoaluminate cement are mainly 3CA· Ba-SO4, β-C_2S and a small amount of celite.
含钡硫铝酸盐水泥的主要矿物组成为含钡硫铝酸钙(简写3CA·BaSO_4)、硅酸二钙(β-C_2S)以及少量的铁相。
4) Ba-containing sulphoaluminate cement concrete
含钡硫铝酸盐水泥混凝土
5) aluminoferrite cement
铁铝酸盐水泥
1.
Research on aluminoferrite cement for application in light wall panel;
铁铝酸盐水泥在轻质墙板中应用的研究
2.
The anchor cement prepared by high performance aluminoferrite cement has a good quality of early strengh, low expansion, cracking resistance and cor rosion resistance.
利用优质铁铝酸盐水泥熟料配制的锚固水泥具有早强、微膨胀、抗裂性能好、耐腐蚀性强等优点。
6) barium-bearing calcium sulfo-ferritealuminate
硫铁铝酸钡钙水泥
补充资料:硫铝酸盐水泥
分子式:
CAS号:
性质:用低品位的矾土和石膏、石灰按适当比例混合磨细后,在1300℃±50℃的回转窑中制得以无水硫铝酸钙(3CaO3Al2O3·CaSO4)和β-2CaO·SiO,占18%~30%为主要矿物的熟料,按与硫铝酸盐的不同摩尔比M加入石膏,可得不同性质的硫铝酸盐水泥。当M=0~1时,为快硬早强水泥,可用于抢修工程;当M=1~2时,可制得微膨胀水泥,用于锚固和刚性防水工程;M>2时,可制成自应力水泥,用于制管工程。