1) Hull mild steel
船用低碳钢
2) low carbon steel for wire drawing
低碳拉丝用钢
1.
According to the collected statistic data of properties and composition of common low carbon steel for wire drawing,the appearing frequency distribution figures of composition and properties are plotted.
根据收集的普通低碳拉丝用钢的性能和化学成分的统计数据 ,绘出化学成分和力学性能的出现频率分布图 ,通过数学分析 ,建立起抗拉强度、下屈服强度、断后延伸率与C ,Si,Mn ,P质量分数的回归方程式。
3) low carbon steel for cold rolling
冷轧用低碳钢
1.
Through the adjusting of composition and optimizing process, low carbon steel for cold rolling has been developed successfully in BaoGang CSP plant,.
通过成分调整和工艺优化,包钢CSP厂成功地研制出适合冷轧生产的热轧低碳钢,这种冷轧用低碳钢晶粒度为8级,屈服强度低于270MPa,冷轧时的轧制力较低,同时通过严格加热炉热工制度和轧辊的换辊制度以及加强了除鳞机的点巡检后,解决了CSP工艺生产的冷轧用低碳钢表面质量差的问题。
4) low carbon carburizing steel
低碳渗碳钢
5) mild steel
低碳钢
1.
Effect of longitudinal magnetic field on microstructure and properties of MIG weld joint of mild steel;
纵向磁场对低碳钢MIG焊焊缝组织及性能的影响
2.
Study of weldability of activating flux for A-TIG welding of mild steel;
低碳钢A-TIG焊活性剂的焊接性研究
3.
Study activating flux for mild steel;
低碳钢A-TIG焊的活性剂研制
6) Low carbon steel
低碳钢
1.
Dissipative structures of inner cracks in low carbon steel during thermal healing;
低碳钢内裂纹热愈合时的耗散结构
2.
Study on Low Carbon Steel Deoxidized by Magnesium Alloy;
低碳钢镁合金脱氧的研究
3.
Analysis on metallurgical effect of low carbon steel in No.1 top-bottom combined blowing converter in Liangang;
涟钢1号顶底复吹转炉低碳钢冶金效果分析
补充资料:拉丝
分子式:
CAS号:
性质:(一)胶黏剂在配制后因超过活性期,胶液部分凝聚所产生的在拉伸情况下成为丝状物的现象。(二)涂料在喷涂时雾化不好,致使涂料不能化为微细的雾滴而呈丝状喷出,所得的涂膜不能流平,出现了拉丝。原因是涂料施工黏度高,稀释剂溶解力差。宜选用适合的溶剂,调整到适宜施工黏度,使涂料在喷涂时能充分雾化,能流平,即可避免此弊病。