1)  martensite [英]['mɑ:tən,zait]  [美]['mɑrtən,zaɪt]
马登斯体,马氏体
2)  martensite [英]['mɑ:tən,zait]  [美]['mɑrtən,zaɪt]
马氏体
1.
Effect of deformation on the temper process of lath martensite;
形变对板条马氏体回火组织的影响
2.
Cold rolling deformation and recrystallization behavior of martensite Ni_(40.5)Co_(32.5)Al_(27) alloy;
Ni_(40.5)Co_(32.5)Al_(27)马氏体合金的冷变形和再结晶行为
3.
Influence of heat treatment on the properties of the heat-resistance martensite stainless steel 0Cr_(17)Ni_4Cu_4Nb;
热处理对耐热马氏体不锈钢0Cr_(17)Ni_4Cu_4Nb性能的影响
3)  martensitic steel
马氏体钢
1.
The microstructure and mechanical properties of China low activation martensitic steel;
低活化马氏体钢的微观结构与力学性能
2.
Introduces forging technology and matters needing attention of valve of martensitic steel 4Cr 10 Si 2Mo, analyses the reason that the steel can ’t be cooled by air, compares forging characteristics with valve of austenitic steel 4Cr 14 Ni 14 W 2Mo and come to the feasiblity of new technology of valve adopting direct extrusion.
介绍了马氏体钢4Cr10Si2Mo气阀的锻造工艺及生产中的注意事项,分析了这种钢不能采用空冷的原因,并且与奥氏体钢4Cr14Ni14W2Mo气阀的锻造特点进行了比较,提出了气阀生产新工艺———正挤压的可行性。
3.
n this research, the characteristic of martensitic steel in abrasion was investigated by using three different test methods.
98%4种合碳量马氏体钢的磨料磨损特性进行了考察。
4)  Half-martensite
半马氏体
5)  martensite steel
马氏体钢
1.
The influence of carbon on microstructure and mechanical property of low-carbon martensite steel was studied by fixing the content of other elements and regulating the content of carbon.
通过固定其它元素的含量,调整碳含量的方式,研究了碳含量对马氏体钢显微组织和力学性能的影响。
2.
The effect of chemical composition and cooling process on microstructure and mechanical properties of specimens taken from the controlled rolled and cooled strips of vacuum melted multiphase and martensite steels were researched.
在实验室用真空感应炉冶炼复相钢和马氏体钢,锻坯、控轧成3 mm厚的板材后采用不同冷却模式进行控制冷却。
3.
about two martensite steels.
对选用的两种马氏体钢的化学成分、力学和物理性能及各项特性进行了系统地介绍。
6)  martensite band
马氏体带
1.
Two kinds of cracking are induced by wide martensite band and carbon - rich band or a phase, all above lead to brittleness of structure which is caused by unsuitable selection of welding consumables and technology.
对某厂30万吨/年乙烯装置裂解汽油二段反应器锻焊接管(A182-F321)与筒体(A387Cr12C12+A240-321)相连角焊缝区裂纹的探伤、检验和分析得出,上述裂纹或位于角焊缝筒体侧熔合区(9例接管),或位于角焊缝金属中(4例接管),两种类型裂纹分别由角焊缝筒体侧熔合区焊缝一侧形成较宽的马氏体带和增碳带引起的脆化(500HV)及角焊缝金属中含量较高的δ铁素体转变成σ相引起的脆化(A_(?)为6-24J)所诱发。
补充资料:马氏体
分子式:
CAS号:

性质:钢中相形态之一。碳在α-Fe中的过饱和固溶体。具有体心正方晶体结构。是一种单相的亚稳组织。钢经奥氏体化后,以超过一定的冷却速度,在较低的温度下发生的马氏体转变产物。马氏体一般呈板条状、透镜片状或二者兼有之。具有较高的硬度和强度。板条状马氏体韧性较好,透镜片状马氏体韧性较差。钢的各种组织中马氏体的比容量大。具有铁磁性,电阻率也比较高。钢的各种组织中马氏体的比容最大。具有铁磁性,电阻率也比较高。通常钢中碳含量直高,马氏体硬度越高。但韧性很差,要经过回火热处理后才能用。通过淬火得到马氏体,是对钢进行强化的重要手段。超低碳铁镍合金中,加入适量的钴、钼、钛等合金元素,可制成高强高韧的马氏体时效钢。