1) tensile heat-distortion
拉伸热变温度
2) drawing temperature
拉伸温度
1.
The results showed the uneveness in thickness of film, drawing temperature, pressure of both roller and infrared heater were main influence factors.
结果表明:薄膜厚度不均、拉伸温度、压辊和红外加热器压力不均及安装检修不当是主要影响因素,通过调整检查可以减少“脱夹”的产生。
3) stretching temperature
拉伸温度
1.
The results show that stretching ratio,stretching temperature,casting conditions and APC system greatly influence the uniformity of film profile.
结果表明,不同拉伸比、拉伸温度、铸片条件及APC系统的控制方式对厚度偏差影响较大。
2.
The transversely stretching temperature and rate have effect on the uniformity of PTFE membrane.
横向拉伸温度和速率均影响薄膜均匀性,温度越高,厚度越薄,孔径越大。
4) isothermal hot tensile test
恒温热拉伸
1.
Steel Group has been studied by means of isothermal hot tensile test.
通过恒温热拉伸的方法研究了太钢生产的00Cr22Ni5Mo3N双相不锈钢的超塑性行为,其中重点研究了该材料的低温超塑性。
5) tensile heat destortion
拉伸热畸变