1) riser wear
隔水管磨损
1.
Based on the consequence analysis of two deepwater riser wear incidents,the wear mechanism for riser system is discussed due to rotation of drillpipe.
结合两起深水钻井隔水管磨损事故后果分析,对钻杆转动造成的隔水管磨损机理进行了探讨和定量评估。
2) casing wear
套管磨损
1.
Method of casing wear prediction for Liuhua mega-extended-reach wells in South China Sea.;
南海流花超大位移井套管磨损预测方法
2.
Summary of casing wear mechanism and test research in deep & ultra-deep well;
深井 超深井中套管磨损机理及试验研究发展综述
3.
In deep drilling process,casing wear is the problem that cannot be ignored.
在深井、超深井钻井过程中,套管磨损有可能导致套管封隔失效和油气井的早期报废。
3) casing abrasion
套管磨损
1.
The complex formations were drilled during the fourth spudding in Sha 84 Well, which resulted in long drilling cycle, multiple trips, and therefore casing abrasion.
沙84井四开井段钻遇复杂地层,钻井周期长,多次起下钻,造成技术套管磨损。
5) boiler tube wear
炉管磨损
6) transducer wall's abrasion
管壁磨损
补充资料:钢筋混凝土循环水管施工
钢筋混凝土循环水管施工
reinforced concrete circulating water pipe construction
gongjln hunn一ngtu xunhuanshu一guan sh一gong钢筋混凝i循环水管施工(reinforced con-erete eireulating water pipe eonstruetion)有现浇和预制两种施工方法。现浇管在挖沟完后,在沟内分段浇筑。预制预应力管在工厂制作,再运到现场敷设。预制管工厂的设备比较简单,如工程地点离工厂较远而该种管子数t多时可将设备搬到现场制造。管子的直径可达3m甚至更大,长度一般为4m。 预制预应力钢筋棍凝土管预制,可用一阶段(展动挤压)工艺或三阶段(管芯绕丝)工艺施工。一阶段工艺系用申立式成型,用加工精密的内外钢套模组合定型,将主钢筋张拉完成后,即浇筑混凝土一次成型,经静定时间后蒸汽养护.三阶段工艺系按上法先浇制混凝土管芯,成型后再在管芯上缠绕预应力钢丝,用机械或电热法张拉,然后再喷盖水泥砂浆保护层,以防钢丝生锈,经水压试验合格后出厂使用。 数设带承插口的钢筋混凝土预制管挖沟徽设.平口对接的钥筋混凝土预制管除挖沟徽设外,还可采用顶管施工(见取水构筑物施工)。挖沟后按设计规定在沟底铺一层黄沙或石子,再用起重机械将预制管逐节吊人沟内、找正位!,在插口上套上橡胶密封圈后,往前一节的承口方向水平加力拉紧,使插口和橡胶圈同时均匀地嵌人承插口内,按此步探依次进行下一节管的安装.橡胶圈本身的直径略大于承插口间尺寸,并有规定的压缩比及防老化剂。在承擂口内侧采用钢衬圈和密封环进行环向水压试验.水压试验的标准按设计和规范要求。安装后进行回坟土,要求在两侧均匀回填分层夯实。 预应力钢筋混凝土管自重较大,在软土地区使用时要做混凝土基础。