1)  LiMn_(2-x-y-z)Tl_xAl_yCr_zO_4
复合尖晶石
1.
The complex LiMn_(2-x-y-z)Tl_xAl_yCr_zO_4 cathode materials with spinel-type structure were synthesized by dopingTl, Al and Cr atoms at the same time and modified solid state reaction, and their physical and electrochemicalproperties were investigated by XRD, SEM, TEM and electrochemical testing.
采用同时掺杂T1、A1和Cr三种金属原子和改进固相反应的方法合成了复合尖晶石正极材料LiMn_(2-x-y-z)Tl_xAl_yCr_xO_4,并采用XRD、SEM、TEM和电化学测试考察了它的物理性质和电化学性能。
2)  complex support of magnesium-alumina spinel
镁铝尖晶石复合载体
3)  spinel-type complex oxide
尖晶石型复合氧化物
1.
The Mn1-x(Li,Ti)xCo2O4 spinel-type complex oxides were prepared by citric acid-ligand combustion method.
用柠檬酸配位燃烧法合成了Mn1-x(Li,Ti)xCo2O4系列尖晶石型复合氧化物催化剂,使用FTIR和XRD方法对催化剂结构进行表征,通过程序升温氧化反应(TPO)技术对这些催化剂在模拟柴油机尾气条件下进行同时消除NOx和柴油碳黑反应的活性评价。
4)  Mg-Fe spinel complex oxide
Mg-Fe尖晶石复合氧化物
5)  spinel composite oxide
尖晶石复合氧化物
6)  Synthesized spinel
合成尖晶石
补充资料:半透明烧结镁铝尖晶石陶瓷
分子式:
CAS号:

性质:又称半透明烧结镁铝尖晶石陶瓷。在0.3~6.5μm范围的线性光透射率大于10%,可见光范围的总透射率约为75%。用镁-铝的盐或氢氧化物的热分解产物为原料,添加少量烧结促进剂氧化钙等。在真空中经1800~1900℃或湿氢气氛中1700℃左右烧结成半透明陶瓷。可用于制作高温电弧、密封外壳、天线窗、红外透射装置等。