说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 尖晶石合成
1)  synthesis of spinel compound
尖晶石合成
2)  Synthesized spinel
合成尖晶石
3)  Pre-synthesized spinel
预合成尖晶石
4)  flux-grown synthetic spinel
助熔剂法合成尖晶石
1.
The conventional methods of the gemmology and the modern instruments of electronic probe, ultraviolet-visible spectrophotometer, Fourier transform infrared spectrometer, cathodoluminescence spectrometer are used to research and analyse the flux-grown synthetic spinel and compare them with the natural spinels.
采用常规的宝石学研究方法以及电子探针、紫外-可见分光光度计、傅里叶变换红外光谱仪和宝石阴极发光光谱仪等现代测试仪器,对助熔剂法合成尖晶石的宝石学特征进行了全面分析,并与天然尖晶石进行了对比。
5)  LiMn_(2-x-y-z)Tl_xAl_yCr_zO_4
复合尖晶石
1.
The complex LiMn_(2-x-y-z)Tl_xAl_yCr_zO_4 cathode materials with spinel-type structure were synthesized by dopingTl, Al and Cr atoms at the same time and modified solid state reaction, and their physical and electrochemicalproperties were investigated by XRD, SEM, TEM and electrochemical testing.
采用同时掺杂T1、A1和Cr三种金属原子和改进固相反应的方法合成了复合尖晶石正极材料LiMn_(2-x-y-z)Tl_xAl_yCr_xO_4,并采用XRD、SEM、TEM和电化学测试考察了它的物理性质和电化学性能。
6)  catalytic removal of NOx
尖晶石类化合物
补充资料:半透明烧结镁铝尖晶石陶瓷
分子式:
CAS号:

性质:又称半透明烧结镁铝尖晶石陶瓷。在0.3~6.5μm范围的线性光透射率大于10%,可见光范围的总透射率约为75%。用镁-铝的盐或氢氧化物的热分解产物为原料,添加少量烧结促进剂氧化钙等。在真空中经1800~1900℃或湿氢气氛中1700℃左右烧结成半透明陶瓷。可用于制作高温电弧、密封外壳、天线窗、红外透射装置等。