1) Exchangeable cavity
可换型芯
2) Rapid-replacing core
快速可换型芯
3) change core quickly
型芯快换
4) fusible core
可熔型芯
1.
By using low melting alloy as fusible core and nylon 66 modified by 30% glass fiber,fistula plastic parts with intricated type were prepared.
以低熔点合金为可熔型芯材料,注射成型形状复杂的30%玻纤增强尼龙66中空塑料件。
2.
The technological process, principles and the key points of technology controlling of the thermosetting plastic by using the fusible core injection moulding were described.
阐述了用可熔型芯注射成型热固性塑料的工艺过程和原理、工艺控制要点。
3.
As a result, the fusible core technique which is similar to investment casting is used in plastic injection molding.
因而在塑料注射成型中引入了类似失蜡铸造的“可熔型芯”制造技术。
6) soluble core
可溶性型芯
1.
The properties of soluble cores are s tudied by experiment in which CaSO4H2O and mSiOnAlO act as matrix and MgSO4·7H2O and P salt act as additives.
实验研究了以石膏和莫来砂为基体、以硫酸镁和P盐为添加剂的可溶性型芯性能,并考虑不同焙烧温度对其性能的影响。
补充资料:Z8612热芯盒射芯机操作规程
1、遵守铸造设备通用操作规程。
2、工作前还必须遵守:
a、
检查设备上行程开关和碰块的位置是否正确,如不正确,必须调整。
b、
接通电源,打开压缩空气伐门,先用手动方法,对各机构逐进行点动试车,然后用自动方法,进行一个循环试车,确认一切正常后,方可进行生产。
3、工作中还必须遵守:
a、
在设备开动后,一个循环未完成时,不许中途调整电器,以免发生误动作,造成设备人身事故;
b、
设备的每一个循环后,必须用喷咀清除芯盒上残存的砂子,并喷涂分型剂;
c、
在未切断电源和所气源前,不准将手伸入芯盒和夹紧器之间的空隙处,或把手放在导轨上,以免发生人身事故。
d、 一般不准空射,如必须空射,一定要把压缩空气伐门关小;
e、 如果用手操作,不准同时操作两个电器开关。
4、工作后还必须遵守:
a、
操纵各个电器开关,使设备各机构恢复到原始位置,然后切断电源和气源;
b、 折下射砂头,清理积砂和粘砂;
c、 清除排气塞内的粘砂;
d、
取下射砂筒,清除缝隙中的粘砂,最后用石蜡涂擦内壁,但不要将缝隙堵塞;
e、 清除闸板上的积砂,并在闸板上涂石墨粉,以减少磨擦;
f、 清除导轨和导杆上的积灰和积砂,并涂上一层润滑油。
2、工作前还必须遵守:
a、
检查设备上行程开关和碰块的位置是否正确,如不正确,必须调整。
b、
接通电源,打开压缩空气伐门,先用手动方法,对各机构逐进行点动试车,然后用自动方法,进行一个循环试车,确认一切正常后,方可进行生产。
3、工作中还必须遵守:
a、
在设备开动后,一个循环未完成时,不许中途调整电器,以免发生误动作,造成设备人身事故;
b、
设备的每一个循环后,必须用喷咀清除芯盒上残存的砂子,并喷涂分型剂;
c、
在未切断电源和所气源前,不准将手伸入芯盒和夹紧器之间的空隙处,或把手放在导轨上,以免发生人身事故。
d、 一般不准空射,如必须空射,一定要把压缩空气伐门关小;
e、 如果用手操作,不准同时操作两个电器开关。
4、工作后还必须遵守:
a、
操纵各个电器开关,使设备各机构恢复到原始位置,然后切断电源和气源;
b、 折下射砂头,清理积砂和粘砂;
c、 清除排气塞内的粘砂;
d、
取下射砂筒,清除缝隙中的粘砂,最后用石蜡涂擦内壁,但不要将缝隙堵塞;
e、 清除闸板上的积砂,并在闸板上涂石墨粉,以减少磨擦;
f、 清除导轨和导杆上的积灰和积砂,并涂上一层润滑油。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。