1.
Organic-inorganic nanocomposite scratch resistant coatings for polycarbonate(PC)were successfully fabricated by evaporation induced self-assembly method.
利用挥发诱导自组装法制备了聚碳酸酯(PC)有机-无机纳米复合耐刮伤涂层,考察了基材处理方式、自组装液组成、涂装工艺等因素对自组装涂层厚度、透明性及耐刮伤性的影响。
4)  evaporation-induced self-assembly(EISA)
挥发诱导自组装法
5)  evaporation-induced self-assembly
蒸发诱导自组装
1.
Preparation of porous silica optical thin films by evaporation-induced self-assembly process;
蒸发诱导自组装法制备多孔二氧化硅光学薄膜
2.
A precursor sol containing tetraethoxysilane (TEOS), surfactant cetyltrimetylammonium bromide(CTAB)-templated and acid/ acid catalyst was prepared by sol-gel and evaporation-induced self-assembly process.
报道采用溶胶—凝胶技术、蒸发诱导自组装法,通过酸/酸二步法控制实验条件,实验中采用表面活性剂十六烷基三甲基溴化氨(CTAB)为模板剂,正硅酸乙酯为硅源,以及二次去离子水,盐酸为催化剂等原料制备前驱体溶胶。
3.
Ordered mesoporous carbon spheres(OMCs) were synthesized by suspension-assist evaporation-induced self-assembly of resorcinol-furfural oligomers and triblock copolymer F127.
以间苯二酚-糠醛低聚物为炭前驱体,三嵌段共聚物F127为结构导向剂,通过悬浮辅助的蒸发诱导自组装乳化成球,高温炭化后得到有序中孔炭球。
6)  induced self-assembly method
诱导自组装
1.
Mesoporous ZnO was synthesized successfully by using the micro-phase ammonia evaporation induced self-assembly method.
采用微相氨蒸发诱导自组装法成功制备了介孔氧化锌,并对其进行氮气的低温吸附和脱附测定其BET比表面积、孔容和孔径分布,结合Low-Angle XRD和TEM表征氧化锌的结构;利用Wide-Angle XRD、HRTEM,、EDS、SAED等表征方法对氧化锌孔壁的物相和晶相进行分析;讨论不同合成条件对介孔氧化锌的孔结构的影响,并探讨微相氨蒸发自组装法制备介孔氧化锌的成孔的机理。