1.
The solid state reaction process of silver behenate and phthalic acid was studied by using X-ray powder diffraction (K value) method in temperature range of 100℃ to 123℃ which is in the development temperature range of photothermographic materials.
在此基础上,采用X射线衍射K值分析法,在光敏热显成像材料热显影温度范围内(100~123℃),研究了山嵛酸银与邻苯二甲酸的固相反应过程。
4) heat-sensitive color-formation
热敏显色
6) hot-water development
热水显影
补充资料:负温度系数热敏电阻陶瓷(见热敏陶瓷)
负温度系数热敏电阻陶瓷(见热敏陶瓷)
thermo-sensitive ceramics with negative temperature coefficient
负温度系数热敏电阻陶瓷thermo一sensitiveeeramies with negative temperature eoeffieient在某一特定温度范围,电阻率随温度的升高而明显减小的热敏陶瓷。简称NTC陶瓷。