1) co-curing agnet
共固化剂
2) blended curing agent
共混固化剂
3) co-curing
共固化
1.
Co-curing Technology Using Water Dispersible Core for the Hollow-Structure Composite Parts
复合材料帽形结构水溶芯模共固化成型工艺研究
2.
Based on the traditional thermoset resin prepreg press molding technology,the press molding co-curing processing method and specification determination of rigid foam cored sandwi.
在分析夹层结构的基础上,概述了常用芯材包括铝蜂窝、NOMEX蜂窝和聚甲基丙烯酰亚胺泡沫塑料的性能和特点,介绍了刚性泡沫夹层结构常用的成型工艺,详细阐述了刚性泡沫夹层结构的模压共固化成型工艺及相关参数的选定。
3.
The soft-mold aided co-curing process of composite grids structures is an advanced techniques with the characters of low cost, high efficient and high quality.
复合材料网格结构软模成型共固化工艺具有低成本,高效率和高质量的特点。
4) co-immobilization
共固定化
1.
Study on culture of chlorella pyrenoidosa with different carbon source for co-immobilization with activated sludge;
用于与活性污泥共固定化的蛋白核小球藻在不同碳源下的培养研究
2.
Study on the co-immobilization of β-galactosidase and glucose isomerase;
共固定化乳糖酶和葡萄糖异构酶的研究
3.
Choosing two kinds of carriers, alginate sodium and chitosan, and inspecting four different kinds of co-immobilized methods, the results showed that the best effect of co-immobilization rooted in choosing alginate sodium as the co-immobilized carrier and the .
本文对单宁酶和β-葡萄糖苷酶进行了共固定化,旨在应用于茶饮料生产中发挥除混与增香之双重功效,从而为纯茶风味茶饮料的生产奠定基础。
5) coimmobilization
共固定化
1.
Studies on coimmobilization of α-Amylase and glucoamylas on celite;
硅藻土共固定化淀粉酶和糖化酶的研究
2.
Studies on Coimmobilization of Heme Oxygenase System and Some Properties;
血红素加氧酶系的共固定化及部分性质研究
3.
And thermostability,storage stability and continuous use stability of the coimmobilization enyme was studied too.
以海藻酸钠为载体,用包埋法共固定α-淀粉酶和糖化酶双酶体系,研究了共固定化过程中双酶的比例、pH值、温度对共固定化后体系稳定性的影响,并探讨了此双酶体系在热稳定性、储藏稳定性、连续使用稳定性方面的效果。
6) curing agent
固化剂
1.
Curing properties of the novel curing agent of epoxy resin;
新型环氧树脂固化剂的性能
2.
Selection of resin and curing agent for PU powder coatings;
聚氨酯粉末涂料树脂及固化剂的选择
3.
Preparation and application of water-soluble bisphenol A-formaldehyde resin as curing agent;
水溶性双酚A型酚醛树脂固化剂的制备及应用
补充资料:120固化剂
N-羟乙基乙二胺又称β-羟乙基乙二胺,俗称120固化剂,结构式H2N(CH2)2NH(CH2)2OH,分子量92.06。无色或淡黄色透明粘性液体,微有氨气味。呈强碱性。有吸湿性。与水、乙醇混溶,微溶于乙酸。能从空气中吸收二氧化碳。低毒.LD504032mg/kg。
用作环氧树脂的室温快速固化剂,参考用量16~18phr,固化条件RT/10h或80℃/3h。
贮存于阴凉、干燥的库房内,防潮。
用作环氧树脂的室温快速固化剂,参考用量16~18phr,固化条件RT/10h或80℃/3h。
贮存于阴凉、干燥的库房内,防潮。