1) solidification rate
凝固率
1.
Based on the theoretical analysis of TiN inclusion precipitation in bearing steel,the saturation solubility curves of TiN inclusion precipitation under different solidification rates was calculated.
通过对轴承钢中TiN夹杂析出的理论分析,得到不同凝固率下TiN夹杂析出溶解度饱和线,据此提出防止TiN夹杂析出的[Ti]、[N]控制范围,同时提出了生产过程中[Ti]、[N]的控制措施。
2) solidification rate
凝固速率
1.
The empirical results indicate that the increase of solidification rate can achieve intermetallic particles reinforced phase with ideal morphological features in Al-Ni alloy.
实验结果表明,提高凝固速率可以使Al-Ni合金获得理想形貌的金属间化合物强化相。
2.
Exporimental results show that the stress- rupture life of DZ22 at 980℃ and 220 MPa was increased from 71 hours and 50 nunutes to 168 hours and 5 minutes at relatively high solidification rate.
本文采用ZMLMC超高梯度定向凝固法(ZMLMC法),研究了两种凝固速率下DZ22合金的高温力学性能和组织。
3.
The dendritic arm spacings and microsegregations of directionally solidified superalloy DZ22 at various solidification rates have been studied with the help of a ZMLMC directional solidification equipment.
采用新研制的超高梯度定向凝固装置,研究了不同凝固速率下定向凝固高温合金DZ22的枝晶臂间距和枝晶偏析。
3) solidication rate
凝固分率
4) critical solidification rate
临界凝固率
5) Soy protein recovery
蛋白质凝固率
6) rate/quick quenching
速率/快速凝固