3) multi-layer composite cathodes
多层复合阴极
1.
The measurements results of polarization curves show that the multi-layer composite cathodes have better electrochemical performance and thermal-cycle stability compared with LSM cathodes.
3MnO3-σ(LSM)在制备及工作温度下与氧化钇稳定的氧化锆(YSZ)电解质发生反应,增大电化学反应电阻,降低SOFC的性能,采用喷涂法在YSZ电解质片的表面制备了LSM-YSZ的多层复合阴极。
5) TiB2 Cathode coatings
TiB2阴极涂层
1.
The solidification of TiB2 Cathode coatings using XD26 under ambient temperature is the technology jointly developed by Shanxi Guanlu Aluminum Co.
介绍山西关铝股份有限公司与中南大学联合开发的“XD26常温固化TiB2阴极涂层” 技术和该技术的工业应用及应用效果,着重论述了该技术及其材料的技术特性。
6) TiB_2 cathode coating
TiB_2涂层阴极
1.
The aim of this paper is to develop large-thickness, long-life TiB_2 cathode coating that possesses excellent performances needed by the drained cell, such as thermal shock resistance, wettability of .
本文的目的就是研制能够满足导流型铝电解槽要求的厚度大、寿命长,同时又具有优良性能(抗热震性、与铝液润湿性、抗腐蚀性、耐磨性和抗钠渗蚀性等)的TiB_2涂层阴极。
补充资料:等离子喷涂羟基磷灰石涂层-钛复合材料
分子式:
CAS号:
性质:是用等离子喷涂技术在医用金属钛或其合金表面加涂羟基磷灰石所制得的医用涂层材料。主要用于承力部位的硬组织修复和替换,如制作人工种植牙、关节柄和接骨板等。由于表面涂层赋予了表面生物活性,植入骨内后能与骨直接形成骨键合,手术中可不用骨水泥固定。为使涂层能在生物环境中保持稳定和涂层-基体界面具有足够的结合强度,要求涂层的羟基磷灰石含量达90%以上并具有高的结晶度。另外,钴基合金也可作为这种涂层材料的基材。
CAS号:
性质:是用等离子喷涂技术在医用金属钛或其合金表面加涂羟基磷灰石所制得的医用涂层材料。主要用于承力部位的硬组织修复和替换,如制作人工种植牙、关节柄和接骨板等。由于表面涂层赋予了表面生物活性,植入骨内后能与骨直接形成骨键合,手术中可不用骨水泥固定。为使涂层能在生物环境中保持稳定和涂层-基体界面具有足够的结合强度,要求涂层的羟基磷灰石含量达90%以上并具有高的结晶度。另外,钴基合金也可作为这种涂层材料的基材。