Based on the method of devitrification by annealing metallic glass, amorphous alloy Fe36Co36B20Si4Nb4 was treated by isothermal annealing at different temperature and different time, the composite with nano-crystal distributed uniformly in the matrix of bulk amorphous alloy was obtained.
利用铜模注射法和铜模吸铸法分别制备出了杆状和管状的非晶态Fe36Co36B20Si4Nb4合金;采用非晶晶化法对非晶态Fe36Co36B20Si4Nb4合金进行了不同保温时间和不同保温温度的等温退火处理,获得了在非晶基体上均匀分布纳米晶的非晶/纳米晶复合材料。
4) rapid solidification
快速凝固法
1.
35RE alloy which was prepared by rapid solidification was processed by hot pressing after ball-milled for different time.
对快速凝固法制备得到的Al-20Si-0。
5) soild-state amorphization
固态非晶化
6) Complete crystallization method from amorphous solids
非晶晶化方法
补充资料:胶乳快速凝固
分子式:
CAS号:
性质: 为缩短胶乳凝固时间,在加有保存剂和稳定剂的鲜胶乳中,加入少量的促凝剂椰子油皂,在凝固剂中加入少量的促凝剂氯化钙,则可促使胶乳尽快凝固成结实凝块。提高促凝剂用量或使用高效的表面活性剂可进一步缩短凝固时间。快速凝固是实现凝固、压片连续化生产、提高制胶效率的必要条件。
CAS号:
性质: 为缩短胶乳凝固时间,在加有保存剂和稳定剂的鲜胶乳中,加入少量的促凝剂椰子油皂,在凝固剂中加入少量的促凝剂氯化钙,则可促使胶乳尽快凝固成结实凝块。提高促凝剂用量或使用高效的表面活性剂可进一步缩短凝固时间。快速凝固是实现凝固、压片连续化生产、提高制胶效率的必要条件。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条