1) (Ni-P)-SiC
(Ni-P)-SiC
2) Ni-P-SiC
Ni-P-SiC
1.
Effect of Heat Treatment on Hardness and Wear Resistance of Electroless Ni-P-SiC Composite Coating;
不同加热方式对Ni-P-SiC化学复合镀层性能的影响
2.
Preparation of Ni-P-SiC electroless composite coating with high wear and corrosion resistance;
化学镀制备高耐蚀耐磨Ni-P-SiC复合镀层
3.
Study on Technology of Electroless Ni-P-SiC (nanometer) Composite Coating;
Ni-P-SiC(纳米)化学复合镀工艺的研究
3) (Ni-P)-SiC-PTFE
(Ni-P)-SiC-PTFE
4) Ni-P/SiC
Ni-P/Sic
5) Ni-P/SiC-PTFE
Ni-P/SiC-PTFE
6) Ni-P-SiC-MoS_2
Ni-P-SiC-MoS_2
1.
Study of Process for Electroless Ni-P-SiC-MoS_2 Composite Plating;
Ni-P-SiC-MoS_2化学复合镀的研究
参考词条
(Ni-P)-SiC复合镀
(Ni-P)-SiC复合镀层
Ni-P/SiC复合镀
Ni-P-SiC化学复合镀
复合化学镀Ni-P-SiC
Ni-P-SiC-MoS_2复合镀层
Ni-P-SiC化学复合镀层
Ni-P-SiC(纳米)化学复合镀
Ni-P/WC、Ni-P/SiC纳米复合镀层
心理形态文化
共时翻译
补充资料:bioactive glass-ceramic composite reinforced by SiC whisker
分子式:
CAS号:
性质:由碳化硅晶须与生物活性玻璃陶瓷复合而成的生物陶瓷复合材料。高强度、高弹性模量、无毒的碳化硅晶须在陶瓷基材中弥散分布,使材料中的裂纹相对均匀,裂纹扩展发生转向和分支;外力作用下碳化硅晶须拔出时产生的拔出效应,使复合陶瓷的弯曲强度达460MPa,断裂韧性达4.3MPa·m1/2,维伯尔系数高达24.7,标志着它是可承力的生物陶瓷复合材料。
CAS号:
性质:由碳化硅晶须与生物活性玻璃陶瓷复合而成的生物陶瓷复合材料。高强度、高弹性模量、无毒的碳化硅晶须在陶瓷基材中弥散分布,使材料中的裂纹相对均匀,裂纹扩展发生转向和分支;外力作用下碳化硅晶须拔出时产生的拔出效应,使复合陶瓷的弯曲强度达460MPa,断裂韧性达4.3MPa·m1/2,维伯尔系数高达24.7,标志着它是可承力的生物陶瓷复合材料。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。