说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 硼硫共渗
1)  boron-sulphurizing
硼硫共渗
1.
By means of analysis, hardness test, abrasion test, this paper studies the effect of boron-sulphurizing on microstructure and properties of boronized layer.
通过金相分析、硬度测试、磨损测定,研究了硼硫共渗对渗硼层组织和性能的影响。
2)  boronsiliconizing
硼硅共渗
1.
The influences of aluminosiliconizing and boronsiliconizing on the microstructure and oxidation resistance of the coatings were researched.
用粉末固体渗法在钼合金表面制备了MoSi2渗层,研究了铝硅共渗和硼硅共渗对渗层的结构和抗氧化性能的影响。
3)  Boron-aluminizing
硼铝共渗
1.
Study on the Self-protective Boron-aluminizing Paste;
自保护硼铝共渗膏剂研究
4)  borovanadizing
硼钒共渗
1.
The results show that borovanadizing layer is more thick and more compact than that of boronizing layer.
采用光学显微镜、扫描电镜和电子探针等检测手段,分析了20钢固体法渗硼和硼钒共渗的渗层组织结构、成分特点及其硬度分布。
5)  boron-vanadizing
硼钡共渗
6)  boronitriding
硼氮共渗
1.
Study on improving the hot forging dies service life of 5CrMnMo Steel of boronitriding;
硼氮共渗提高5CrMnMo钢热锻模使用寿命的研究
2.
Research for the Structures, Properties and the Mechanism of Borosulphurizing and Boronitriding;
硼硫、硼氮共渗组织和性能及其机理的研究
3.
Microstructure of the boronitriding layer on austenitic stainless steel and the transition zone between the layer and matrix has been examined.
研究了奥氏体不锈钢硼氮共渗渗层及过渡区组织结构,并对共渗机理进行了探讨。
补充资料:碳氮硼三元共渗
分子式:
CAS号:

性质:碳氮硼三元共渗是使钢制工件同时渗入碳、氮、硼三种元素的化学热处理工艺。共渗后渗层的硬度较渗硼为低(HV600~1000)。碳氮硼三元共渗如用于石油机械易损零件,能提高使用寿命。碳氮硼三元共渗后空冷即可得到HV750的硬度,对于上述钢材制造的薄小工件,可以省去淬火工序。碳氮硼三元共渗也可以在气体介质中进行,例如用尿素(2500g)、甲醇(8L)、硼酸三甲酯(5L)、丙酮(6L)的混合渗剂滴入840~860℃的井式渗碳炉中,保温3~5h后,在低碳合金渗碳钢上可得到0.4~0.6mm渗层,表面硬度达HRC63~65,甚至更高。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。