1) sintered carbon steel
烧结碳钢
1.
The repeated impact method with low energy,was adopted for measuring the fracture toughness of sintered carbon steels with sample size of 12mm×12.
5mm烧结碳钢的断裂韧性KIC值。
2) carbusintering
[,kɑ:bju'sintəriŋ]
渗碳烧结
1.
Study on Behavior of Ferrous Materials in Carbusintering;
通过热处理进一步提高了材料的强度,且渗碳烧结材料经热处理后力学性能更优。
3) carbon sintering
正碳烧结
1.
The technology and principle of adding carbon sintering are introduced.
概述了国内外梯度结构硬质合金的发展,介绍了采用正碳烧结工艺制备WC-Co梯度结构硬质合金的工艺和梯度形成机理,并列举了粘结相梯度结构硬质合金的实际应用,展望了该合金的应用开发前景。
2.
The technology, principle of adding carbon sintering are introduced, and the applying and prospects of gradient cemented carbides are discussed.
概述了国内外梯度硬质合金的进展,介绍了采用正碳烧结工艺来制备WC-Co梯度结构硬质 合金的工艺和基本原理,列举了合金的实际应用领域,指出了该合金的应用开发前景。
4) carburizing sintering
碳化烧结
5) Sintered steel
烧结钢
1.
Influence of alloy elements Ni、Mo、W and copper infiltrated on wear resistance of sintered steels;
合金元素Ni、Mo、W及熔渗铜对烧结钢耐磨性的影响
2.
The effect of Si Mn (SM) master alloy content on mechnical properties of Fe SM C sintered steel was investigated.
运用 L1 6 (4 4 × 2 3)正交设计的实验方法 [1 ] ,研究了 SM(Si- Mn)母合金含量对 Fe- SM- C烧结钢力学性能的影响。
3.
4C sintered steel has been studied.
4C烧结钢性能与组织的影响。
补充资料:烧结碳钢
分子式:
CAS号:
性质:采用粉末冶金方法制得的碳素钢材料。强度一般为0.7GPa左右,硬度和耐磨性均优于烧结铁。通过热处理和表面硬化处理可以进一步提高其力学性能。适于制造齿轮等机械零件。原料采用铁粉和石墨粉,在0.7~1.5GPa的压力下冷压成形,然后在发生炉煤气的保护下加热至1100~1400℃烧结1~4h。烧结碳钢的组织和性能随含碳量不同而异。
CAS号:
性质:采用粉末冶金方法制得的碳素钢材料。强度一般为0.7GPa左右,硬度和耐磨性均优于烧结铁。通过热处理和表面硬化处理可以进一步提高其力学性能。适于制造齿轮等机械零件。原料采用铁粉和石墨粉,在0.7~1.5GPa的压力下冷压成形,然后在发生炉煤气的保护下加热至1100~1400℃烧结1~4h。烧结碳钢的组织和性能随含碳量不同而异。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条