1) Nickel Chromium alloy cast iron
低镍铬铸铁
2) nickel-chromium cast iron
镍铬铸铁
3) low-Cr cast iron
低铬铸铁
1.
The WC and low-Cr cast iron composite layer samples were prepared by casting-penetrating process to improve the wear resistance of the low-Cr cast iron.
为进一步提高低铬铸铁的耐磨性,利用铸渗工艺采用膏块法制备了WC/低铬铸铁复合铸渗层试样。
2.
VS+Ti+Zn compound inoculant plays a favorable role in improving property process of low-Cr cast iron.
在低铬铸铁改性处理中,VS+Ti+Zn复合孕育剂起着良好的孕育处理作用。
4) Low chromium cast iron
低铬铸铁
1.
Worn morphology of low chromium cast iron grinding balls used in wet mill in Dexing copper mine was analyzed with SEM(scanning electrical microscope).
低铬铸铁磨球存在切削、凿削、冲击坑及腐蚀坑等多种磨损形貌 ,观察分析后可知 ,欲进一步降低耗球量 ,不仅要提高磨球的硬度 ,而且要提高磨球材质的耐蚀
2.
In this paper the structure of low chromium cast iron (CrO2) on cast condition has been researched The results show that the structure is composed of eutectic carbide Fe 3C,(Cr,Fe) 7C 3 and sorbite The type of carbide is not changed but high hardness can be acquired by heat treatmen
研究了CrO2低铬铸铁的铸态组织结构,结果指出,铸态组织为Fe3C、Cr7C3型共晶碳化物+索氏体基体组成。
3.
The wear resistance of low chromium cast iron with the addition of 0.
结果表明:由于钒、铁合金元素在低铬铸铁中的有益作用,使其硬度、韧性与耐磨性均比不加钒、钛的高。
5) middle Cr-Ni cast iron
中铬镍铸铁
6) high Ni Cr cast iron
高镍铬铸铁
1.
The technical parameters and production process of the combine roller made from high Ni Cr cast iron by centrifugal casting were intruduced in detail.
详细介绍了离心铸造高镍铬铸铁复合辊套内外层金属铸造工艺参数及整个铸造生产过程。
补充资料:镍硬铸铁
分子式:
CAS号:
性质:以镍铬为主的白口铸铁。镍硬1号含(%):C3.0~3.6, Si0.3~0.5, Mn0.3~0.7, Ni3.3~4.8, Cr1.5~2.6; 镍硬2号含(%):C≤2.9,Si 0.3~0.5, Mn0.3~0.7, Ni3.3~5.0, Cr1.4~2.4; 镍硬4号含(%):C2.6~3.2, Si1.8~2.0, Mn0.4~0.6, Ni5.0~6.5, Cr8.0~9.0。它们均以马氏体为主,尚有一定的贝氏体和奥氏体。它们的硬度较高,镍硬1号为HRC53~61,镍硬2号为HRC52~59,镍硬4号为HRC53~63。镍硬铸铁最好用电炉熔化,便于控制成分和浇注温度,通常均需进行热处理。镍硬铸铁广泛用于低抗磨损,如轧辊、衬板、磨煤机的磨辊和磨环、输送管道、杂质泵过流部件等。
CAS号:
性质:以镍铬为主的白口铸铁。镍硬1号含(%):C3.0~3.6, Si0.3~0.5, Mn0.3~0.7, Ni3.3~4.8, Cr1.5~2.6; 镍硬2号含(%):C≤2.9,Si 0.3~0.5, Mn0.3~0.7, Ni3.3~5.0, Cr1.4~2.4; 镍硬4号含(%):C2.6~3.2, Si1.8~2.0, Mn0.4~0.6, Ni5.0~6.5, Cr8.0~9.0。它们均以马氏体为主,尚有一定的贝氏体和奥氏体。它们的硬度较高,镍硬1号为HRC53~61,镍硬2号为HRC52~59,镍硬4号为HRC53~63。镍硬铸铁最好用电炉熔化,便于控制成分和浇注温度,通常均需进行热处理。镍硬铸铁广泛用于低抗磨损,如轧辊、衬板、磨煤机的磨辊和磨环、输送管道、杂质泵过流部件等。