Study on Wear Characteristics of SiC_P/ZrO_2-MoSi_2 Nanocomposite Ceramic;
用磨损对比试验对无润滑条件下SiCP/ZrO2-MoSi2纳米复合陶瓷的磨损特性进行了分析。
3)  SiCP/MoSi2 composite
SiCP/MoSi2复合材料
1.
The oxidation resistance at 800~1 200℃ of hot-pressed SiCP/MoSi2 composite with various volume fractions of in-situ produced SiC particulate was investigated using TGA,XRD,SEM and oxidation kinetic analysis.
结果表明,SiCP/MoSi2复合材料的抗氧化性能强于纯MoSi2材料;适量原位SiC颗粒的生成可以提高SiCP/MoSi2复合材料的抗氧化性能;材料氧化反应生成的SiO2层的致密性影响其氧化活化能及抗氧化性能,SiO2层越致密,氧化活化能越高,抗氧化性能越好。
2.
MoSi2 and SiCP/MoSi2 composites reinforced with different volume fractions of in-situ SiC particles were fabricated by means of in-situ reaction and hot press synthesis after wet mixing pure powders of Mo,Si and C.
以钼、硅、碳粉末为原料,采用湿法混合和原位反应热压一次复合工艺制备了MoSi2以及含不同体积分数原位SiC颗粒的SiCP/MoSi2复合材料,并研究了原位SiC颗粒对该材料室温断裂韧度的影响。
4)  molybdenum disilicide
MoSi2
1.
Molybdenum disilicide was synthesized successfully from element Mo and Si powders using self -propagating high - temperature synthesis technology.
以Mo粉和Si粉为原料,通过自蔓延高温燃烧合成(SHS)的方法成功地制备了MoSi2材料。
2.
Vikers microhardness indentation and single edge notched beam specimen techniques were evaluated, and the modified equation was presented in the measurement of fracture toughness of molybdenum disilicide matrix composites.
对压痕法和单边切口梁法所测MoSi2 基复合材料的断裂韧性作了研究和分析 ,提出了压痕法测量MoSi2 基复合材料断裂韧性的计算修正式。
5)  MoSi_2
MoSi2
1.
This paper reviews the current research status and the development trend of MoSi_2 material and its composites.
综述了MoSi2及其复合材料的国内外研究现状和发展趋势。
2.
Changes of MoSi_2 coatings by Plasma Spraying at different heat treating process were studied.
研究了等离子喷涂单一MoSi2涂层在不同的热处理工艺条件下发生的变化,结果表明650℃保温1 h,试样出现粉化现象,验证了“Pesting”现象;750℃保温1 h试样背面出现Mo的氧化物晶体,对混合涂层的透射电镜观察证实了MoSi2的热障涂层中起到了自愈合作用。
3.
8%La_2O_3-Mo_5Si_3/MoSi_2 composites at 1200 ℃ in air was investigated.
8%La2O3-Mo5Si3/MoSi2复合材料在1200℃空气中的高温氧化行为。
6)  MoSi 2
MoSi2
1.
The uniform dispersing processing of ZrO 2(n) /MoSi 2 composite powders and SiC (W) /ZrO 2(n) /MoSi 2 composite powders prepared by mixing with multiphase suspension were also discussed.
介绍了SiC晶须分散工艺,探讨了多相悬浮液混合法制备ZrO2 (n) MoSi2 复合粉体及SiC(W) ZrO2 (n) MoSi2 复合粉体的均匀混合工艺。
2.
The sintering tempera ture of MoSi 2 by MA is at least lower about 250℃than that by SHS.
利用粉末烧结理论对比分析了机械合金化(MA)和高温自蔓延(SHS)合成的MoSi2粉末的烧结性能,并阐明了原因。
3.
Microstructure of the laser cladding molybdenum silicides composite coatings consists of the primary dendritic MoSi 2,plate-like iron-molybdenum-silicide (FeMoSi) and the interdendritic MoSi 2α eutectic struc.
以Mo -Si合金粉末为原料 ,采用激光熔覆技术在奥氏体不锈钢 1Cr1 8Ni9Ti表面上制得了由初生MoSi2 树枝晶、块状FeMoSi初生相及枝晶间MoSi2 /α片层状共晶组织组成的难熔金属硅化物高温复合材料涂层。