1)  refractory zinc oxide minerals
难选氧化锌矿
1.
The ammonia leaching process of zinc oxide is thermodynamically analyzed based on the feature of refractory zinc oxide minerals.
针对难选氧化锌矿的特点 ,对氧化锌矿氨浸过程进行热力学分析。
2)  refractory oxidized leadzinc ore
难选氧化铅锌矿
1.
Based on the characteristics of refractory oxidized leadzinc ore and the technical requirement of desliming before oxide zinc flotation,the ore grinding process and method is improved to reduce the slime produced during grinding and has reached some results.
针对兰坪难选氧化铅锌矿矿石特点及氧化锌浮选前必须脱泥的技术要求,为了减少磨矿过程中产生矿泥,进行了磨矿工艺改进,取得了初步效果,本文对碎磨工艺及磨矿方式进行探讨。
3)  refractory zinc oxide ore
难选氧化锌矿石
4)  refractory oxidized ore
难选氧化矿
5)  Uneasily mining and processing ore
难采难选氧化矿
6)  refractory oxidized copper ores
难选氧化铜矿石
1.
The chelating collector B130 has some important adventages, such as stronger collecting property and better selectivity for refractory oxidized copper ores, and is capable of convenient utility.
螯合捕收剂B130浮选难选氧化铜矿石具有捕收力强、选择性好、使用方便等优点,尤其是对含铁高、泥化严重的矿石更是如此。
补充资料:低品位氧化锌矿富集


低品位氧化锌矿富集
concentration of zinc from lowgrade zinc oxide ore

  理含锌大于7.8%、含铅大于1.2%的氧化锌矿,产出含锌60%、含铅10%的粗氧化锌,而后与硫化锌精矿混合后进行烧结焙烧、鼓风炉炼锌和粗锌精馏,产出精馏锌。该企业的设计年处理氧化锌矿能力为45万t。 烟化炉烟化法是把空气和粉煤吹入烟化炉内含锌的熔渣中,使熔渣中的氧化锌还原成锌蒸气挥发出来,在炉内上部空间被吸入的空气再氧化成氧化锌,并以粗氧化锌粉形态被收集。中国云南会泽铅锌矿采用粉矿压团、炼铅鼓风炉还原法产出粗铅、炉渣烟化炉烟化产出含锗氧化锌、用湿法炼锌方法生产金属锌和锗,处理含锌8%一15%、铅3%~5%、锗0.003%一0.0045%的氧化锌矿生产金属锌和锗。设计年生产能力为电锌12o00t,粗铅sooot;烟化炉挥发率:铅96%,锌99.21%,锗99.1%;粗氧化锌含锌60%、铅11%一14%、锗0 .03%一0.04%。d一P一nwe一yonghuox.n kuong fuJ-低aaa位氧化锌矿富集(Coneentrati()n()f zin。from low一grade zine oxide ore)用火法富集法提高氧化锌矿或含锌物料品位的锌炉料准备力一法,低品位氧化锌矿物的可选性差,多采用火法富集产出粗氧化锌,再进一步提取金属锌。火法富集的方法有回转窑挥发法和烟化炉烟化法。 回转窑挥发法是用碳质还原剂于约1273K温度下,将置于回转窑内的低品位氧化锌矿还原,产出的金属锌以蒸气形态挥发出来后,在烟气中氧化并带至收尘设备中,经收集得到含锌品位符合冶炼要求的氧化锌粉。意大利的维斯麦港铅锌联合企业‘The IsFComplex at porto Vesrne)采用回转窑还原挥发法处
  