1) fluoro rubber F_(2314)
氟橡胶F2314
2) fluororesin F2314
F2314氟树脂
1.
Samples of fluororesin F2314 and polymer bonded explosive (PBX) using F2314 as binder were aged under different condition.
对F2314氟树脂及以F2314为粘结剂的高聚物粘结炸药(PBX)进行了老化试验,老化前后检测了F2314的结晶度、贮存模量、损耗因子及以F2314为粘结剂的PBX的力学性能。
3) fluorine rubber
氟橡胶
1.
Adhesion properties and mechanism of epoxy adhesive in bonding fluorine rubber to metal;
氟橡胶-金属黏接用环氧树脂胶黏剂的黏接性能与黏接机理
2.
Advance in bonding metal to fluorine rubber;
氟橡胶与金属黏接的研究进展
3.
We adopted a newly epoxy resin prepared by 4,4'-dihydroxydiphenyl sulfone and epoxy E-51,developed a newly epoxy adhesive for bonding fluorine rubber to metal,studied adhesion properties and endurance of the adhesive systematically.
用4,4’-二羟基二苯砜与E-51反应制备的树脂配制了可直接用于氟橡胶与金属粘接的新型环氧树脂胶粘剂,系统研究了胶粘剂的粘接性能及耐久性。
4) fluorosilicone rubber
氟硅橡胶
1.
Development of domestic fluorosilicone rubber;
国内氟硅橡胶的研究进展
2.
Preparation of fluorosilicone rubber with good adhesive properties;
具有良好粘接性能的氟硅橡胶的研制
3.
Effects on the heat resistant properties of copolymerized fluorosilicone rubber to metal oxide;
金属氧化物对共聚氟硅橡胶耐热性能的影响
5) fluoroether rubber
氟醚橡胶
1.
Property and application of fluoroether rubber;
氟醚橡胶的性能及其应用
2.
The compatibility of fluoroether rubber and fluorosilicone rubber blends has been studied using vulcameter,dynamic mechanical thermal analysis(DMTA)and differential scanning calorimetry(DSC).
通过硫化仪、动态机械热分析仪和示差扫描量热仪,考察了氟醚橡胶与氟硅橡胶的共混相容性。
3.
The effects of different amounts of graphite,carbon fiber,PTFE and their blending on the properties of friction and abrasion of fluoroether rubber were studied.
研究了石墨、碳纤维和聚四氟乙烯不同用量和三者并用对氟醚橡胶摩擦磨损性能的影响,并用SEM对橡胶磨损表面形貌进行了分析。
6) fluororubber
氟橡胶
1.
Study on curing kinetics of epoxy adhesive for bonding fluororubber to metal;
氟橡胶-金属粘接用环氧胶固化动力学研究
2.
Current situation and application for the fluororubber at home and abroad;
氟橡胶国内外发展现状及应用
3.
Properties of fluororubber/methyl vinyl silicone rubber blends elastomer
氟橡胶/甲基乙烯基硅橡胶共混弹性体的性能
补充资料:聚酯氟橡胶
分子式:
CAS号:
性质:是含氟二元醇(如六氟-1,5-戊二醇)和二元酸(如己二酸)的缩聚物。拉伸强度13.7~20.5MPa,伸长率100%~500%,玻璃化温度约-72℃,使用温度达185℃。耐溶剂、耐低温性好。柔软性类似天然橡胶。用于制造航空燃料桶。
CAS号:
性质:是含氟二元醇(如六氟-1,5-戊二醇)和二元酸(如己二酸)的缩聚物。拉伸强度13.7~20.5MPa,伸长率100%~500%,玻璃化温度约-72℃,使用温度达185℃。耐溶剂、耐低温性好。柔软性类似天然橡胶。用于制造航空燃料桶。