1) volume expansibility
吸水膨胀率
1.
The results showed that the volume expansibility of water swollen rubber increased with the increasing amounts of water-Absorbing resin, but its physical properties decreased.
结果表明,吸水膨胀橡胶的吸水膨胀率随吸水树脂用量增加而增大,拉伸强度和拉断伸长率随吸水树脂用量增加而降低;随炭黑用量增加,物理机械性能提高,但体积膨胀率明显下降;建立的数学模型能较好地拟合炭黑和吸水树脂用量与胶料各项性能之间的关系。
2.
The results show that the volume expansibility of water swelling rubber increases with the increase of amounts of water-absorbing resin,but its physical properties decreases.
结果表明 :吸水膨胀橡胶的吸水膨胀率随吸水树脂用量增加而增大 ,拉伸强度和扯断伸长率随吸水树脂用量增加而降低 ;硫化剂用量越多橡胶吸水膨胀率越小 ;橡胶吸水膨胀率随白炭黑用量增加而略有上升。
2) Thickness swelling rate
吸水厚度膨胀率
1.
The radial and tangential thickness swelling rates of compressed Chinese fir wood were determined and analyzed in different water temperature and interval.
测定和分析了杉木压缩木在不同水温、不同时段的径向和弦向吸水厚度膨胀率 结果表明,不同条件下,径向和弦向吸水厚度膨胀率随时间变化的速度和幅度不同,达到径向和弦向最大吸水厚度膨胀率的时间也不同 该研究结果为杉木压缩木的生产和利用提供了科学的理论依
3) TS
吸水厚度膨胀率
1.
THE EFFECTS OF ALL MAIN MANUFACTURING FACTORS ON THE THICKNESS SWELLING IN PARTICLEBOARD;
制造工艺因素对刨花板吸水厚度膨胀率的影响
2.
By tracking test on the different density particleboard made of Populus ussuriensis and Larix gmelini ,and the different thickness wood of Populus ussuriensis and Larix gmelini , this paper showed the thickness swelling equation of particleboard and wood are quite the same and coincide rather well with the theoretical deduction, that is TS(t)=a-b e -t/τ .
对不同密度杨木刨花板、落叶松刨花板及不同厚度杨木、落叶松在不同方向的吸水厚度膨胀率进行追踪测试 ,然后进行回归拟合 ,结果表明 ,刨花板和木材的吸水厚度膨胀率方程与理论推导结果能很好的吻合 ,方程的数学形式都为 :TS(t) =a -be-t τ。
3.
We analyzed the effects of hot pressing time,resin content,board density,and ratio of wood shavings to tobacco stems on the particleboard properties including modulus of rupture(MOR),internal bonding strength(IB)and thickness swelling rate of water absorption(TS).
初步探讨了实验室条件下烟秆/木材刨花板的生产工艺,研究了热压时间、施胶量、密度、木刨花加入量等因素对板材的静曲强度、内结合强度、吸水厚度膨胀率的影响。
4) thickness swelling
吸水厚度膨胀率
1.
Influence of thickness swelling on the quality stability of laminate floor covering;
吸水厚度膨胀率对强化木地板质量稳定性的影响
2.
A test study was made on the influence of water temperature on the thickness swelling of medium density fireboard (MDF).
通过验证试验,探讨了水温变化对中密度纤维板吸水厚度膨胀率的影响程度,并对日常检测中如何保证水温符合检测要求提出了相应的建议。
3.
The study was conducted to make compressed bamboo by hot compressing microwave-softened bamboo of four different ages, during which the effect of compression rate, compress temperature and compress time on thickness swelling and recovery rate from compressive deformation was analyzed through orthogonal experiments.
运用正交分析法分析压缩率、热压温度、热压定型时间对密实化竹材的吸水厚度膨胀率和压缩变形恢复率的影响。
5) water Swelling
吸水膨胀
1.
Synthesis and Evaluation of Water Swelling Polymer Plugging Agent
吸水膨胀型聚合物堵漏剂的合成与评价
2.
Since it has a high swelling rate but no crack and dispersion after water swelling,the composite can be used as water-swelling waterproof material.
该复合材料中膨润土的含量可达到70%,其吸水膨胀速度快,浸水24 h后,吸水体积膨胀率可达到其最大吸水体积膨胀率的80%以上,吸水体积膨胀率较高,吸水膨胀后不开裂,不分散,可以被用做吸水膨胀类型防水材料。
6) water-swellable NR
吸水膨胀NR
1.
Preparation and properties of water-swellable NR;
吸水膨胀NR的制备与性能研究
补充资料:吸水膨胀密封胶条
分子式:
CAS号:
性质:橡胶密封胶条的一种。胶料中配合有吸水材料,在干燥状态下与一般实心密封胶条并无差别,当与水接触时立即吸收水分体积迅速膨胀并充塞于缝隙各空间,堵塞、切断水流通道而达到止水密封效果。常用于房屋建筑及地下工程接缝部位止水密封。
CAS号:
性质:橡胶密封胶条的一种。胶料中配合有吸水材料,在干燥状态下与一般实心密封胶条并无差别,当与水接触时立即吸收水分体积迅速膨胀并充塞于缝隙各空间,堵塞、切断水流通道而达到止水密封效果。常用于房屋建筑及地下工程接缝部位止水密封。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条