1) rib-pressing die
压筋凹模
2) stamping cavity die
冲压凹模
3) extrusion female die
挤压凹模
1.
Optimum design of combined extrusion female die;
组合式挤压凹模的优化设计
4) cold stamping female die
冷压凹模
1.
The fracture analysis result of the failure cold stamping female die shows that the little crack of the cold stamping die belongs to fatigue crack,and that at the same time the non-uniform distribution of the carbide can introduce the crack origination and the low-cycle fatigue rupture failure of die.
由冷压凹模断口形貌失效分析结果表明,凹模内壁微小裂纹属于疲劳裂纹,同时凹模材质CrWMn钢中的所存在的碳化物不均匀性诱发了裂纹的产生,导致模具在低周疲劳状态下发生断裂失效。
5) Beading die
压筋模
6) punch for rib-pressing
压筋凸模
1.
The rib-pressing pressure and working stroke of the punch for rib-pressing were calculated.
对壳体压筋进行工艺分析,计算压筋成形力及压筋凸模工作行程,介绍组合压筋模具结构设计,模具结构比较复杂,但生产效率高,操作简单、方便,降低了生产成本,满足大批量生产的要求。
补充资料:凹模壁厚及凹模垫板尺寸
型腔壁部投影面积 壁 厚, 毫 米
F, 厘米2 h1 h2 h3 h4 h5
<5 15~20 30~40 <=10 15~20 30~40
>5~10 20~25 40~50 10~15 20~25 40~55
>10~50 20~30 50~60 15~20 20~30 55~65
>50~100 30~35 60~75 20~25 30~40 65~70
>100~200 35~40 75~85 25~30 40~50 70~75
>200 >40 >85 30~35 50~60 >80