1) multitrack overlapping
多道搭接
1.
Residual stress in the upper layer of multitrack overlapping laser-clad WF218 Nickle-based coating presents as tensile stress,while in the transition zone between coating and substrate,the residual stress presents as compressive stress.
为了克服多道搭接激光熔覆层的开裂问题,分析了熔覆层与基体材料之间的力学关系,建立了激光熔覆层残余应力测试方法,推导了残余应力的计算公式。
2) overlapping clad
多道搭接
1.
The structure and hardness as well as their influential factors of laser\|clad Ni+Cr 3C 2 composite coatings with a single clad track (SCT) and overlapping clad tracks (OCTs) have been investigated.
对激光单道与多道搭接熔覆Ni+Cr3C2 复合涂层的组织、硬度及其影响因素进行了研究。
3) overlapped road
道路搭接
5) interpass cold lap
焊道内冷搭接
6) multiple rivet lap
多行铆钉搭接