1) side groove
侧凹
1.
The structure and working process of injection mould for side groove plastic parts were introduced with two parts as examples,and the key problem of forcibly demoulding was analyzed.
通过实例介绍两种带有侧凹(或侧凸)的塑料制品强制脱模的注射模典型结构及其工作原理,并分析了强制脱模应注意的事项。
2) internal concave
内侧凹
1.
Design of injection mould for a part with internal concave;
带内侧凹塑件注射模设计
3) Undercut Feature
侧凹特征
1.
A new graph-based recognition method of undercut features from molded part was proposed.
提出一种基于图的注塑产品侧凹特征识别方法:首先将产品属性面邻接图中的节点和边进行属性扩展,以形成产品的扩展属性面邻接图;在此基础上,应用扩展属性面邻接图对凹、凸及通孔三种类型的侧凹特征进行描述,并采用子图匹配的方式将侧凹特征的子图从产品属性面邻接图中识别出来;对于识别出的侧凹特征,特征方向可采用可视图的方法确定,并通过分析识别出的侧凹特征的特征方向来最终确定产品的优化脱模方向。
4) outer seg
外侧凹痕
5) outside annular concave
环形外侧凹
1.
According to the structure and technology characters of the plastic part with outside annular concave,the bayonet Half is used in the injection mould.
根据带环形外侧凹开关件的结构和工艺特点,在模具设计中采用插入式哈夫块的侧向抽芯机构成型环形外侧凹,使模具结构简单、加工方便;采用潜伏式浇口的滞后顶出,减少了模具使用中潜伏式浇口处的堵塞,延长了模具的寿命。
6) Loose Core on Inboard Concave
内侧凹抽芯
参考词条
补充资料:凹模壁厚及凹模垫板尺寸
型腔壁部投影面积 壁 厚, 毫 米
F, 厘米2 h1 h2 h3 h4 h5
<5 15~20 30~40 <=10 15~20 30~40
>5~10 20~25 40~50 10~15 20~25 40~55
>10~50 20~30 50~60 15~20 20~30 55~65
>50~100 30~35 60~75 20~25 30~40 65~70
>100~200 35~40 75~85 25~30 40~50 70~75
>200 >40 >85 30~35 50~60 >80