1)  scaling conditions
结垢条件
2)  heat exchanger components scaling
换热元件结垢
3)  crystallization conditions
结晶条件
1.
The relations between phase transitions and can-breaking of CTCBE and CB under different crystallization conditionswere investigated.
研究不同冷却结晶条件下CTCBE和CB的晶型衍变与胀罐的关系。
2.
The static osmotic membrane crystallization of papain was studied,and optimal crystallization conditions were chosen.
用中空纤维微孔疏水膜进行木瓜蛋白酶的渗透膜结晶,研究温度和不同pH的缓冲溶液对木瓜蛋白酶静态渗透膜结晶的影响,优化木瓜蛋白酶渗透膜结晶的结晶条件。
3.
The influences of various crystallization conditions on the shape and quality of lysozyme crystals were investigated and some high quality crystals obtained after the crystallization conditions were optimized.
用动态膜结晶法对溶菌酶结晶进行研究,考察了各种结晶条件对溶菌酶晶形和膜通量的影响,并对结晶条件进行优化,得到了质量较高的溶菌酶晶体。
4)  sintering conditions
烧结条件
1.
The influence of the La and Y relative concentration and sintering conditions were studied respectively.
分别研究了La和Y双施主掺杂以及烧结条件对材料PTC性能的影响,实验表明,以La和Y进行双施主掺杂可使材料的室温电阻进一步降低,升阻比提高。
5)  sintering condition
烧结条件
1.
Effects of sintering condition on property of porous HA bioceramic implant;
烧结条件对多孔HA生物陶瓷种植体性能的影响
2.
Their average coefficients of thermal expansion were tested from 20~1000℃, and the effect of sintering conditions on their thermal expansion property was investigated.
将用共沉淀法合成的NZP型二元固溶体Ca1-xBaxZr4(PO4)6(0≤x≤1,简称CBZP)系列粉体分别添加ZnO和MgO为烧结助剂,在80MPa下干压成型,分别经1100~1300℃无压烧结30~120min,制成CBZP系列陶瓷材料,测定了20~1000℃的平均线膨胀系数,着重研究了烧结条件对该系列陶瓷热膨胀性能的影响。
3.
The ceramic of CBZP series were made by pressing and sintering, the affection of sintering conditions to mechanic character were investigated.
将CBZP系列粉体干压成型 ,用无压烧结制成CBZP系列陶瓷 ,研究了烧结条件对致密化程度及其力学性能的影响 。
6)  frost formation condition
结霜条件
补充资料:结垢控制
分子式:
CAS号:

性质: 又称结垢抑制(scale inhibition)。抑制垢生成的物理或化学的方法。控制方法有:(1)减少致垢物质的采源,包括水的软化、降低水中悬浮物、防止环境污染、控制水中菌藻类的生长和金属的腐蚀等;(2)循环冷却水的内部处理,包括排污、酸化、磷化、碳化以及化学药剂处理等。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。