1) incipient melting
初熔
2) initial melt
初熔体
1.
The rapid spreading out of the initial melt through adhering layer seems to be essential to achieve solid bonding phase in microstructure in sinter.
渗透性测试可用来观察最初熔体的扩展情况。
3) Beginning melting curve
初熔曲线
4) Initial melting
初始熔融
5) primary smelting
初步熔炼
6) incipient melting temperature
初熔温度
1.
The incipient melting temperature of DZ68 alloy was confirmed between 1 240 ℃ and 1 260 ℃ by metallographic analytical method.
运用金相分析法确定了DZ68合金的初熔温度范围为1 240~1 260℃。
补充资料:熔盐电解法生产铌粉(见熔盐电解法生产钽粉)
熔盐电解法生产铌粉(见熔盐电解法生产钽粉)
production of niobium powder by molten salt electrolysis
rongyand+onjlefa ShengChan n.fen熔盐电解法生产妮粉(produetion。fn;obi-um powder by molten salt eleetrolysls)见熔盐电解法生产担粉。