1) alloying extent
合金化程度
1.
The Pt-Ru particles of the Pt-Ru/CMK-3 catalyst were found to be with high alloying extent,small average size and low relative crystallinity when the Pt-Ru/CMK-3 catalysts was prepared with the general chemical reduction method in the mixture solution of tetrahydrofuran(THF)and H2O.
与在纯水中制得的Pt-Ru催化剂相比,其Pt-Ru粒子的合金化程度高、平均粒径较小且相对结晶度低,因此该催化剂对甲醇氧化的电催化活性远高于在纯水中制得的Pt-Ru催化剂。
2.
The Pt-Ru particles of the Pt-Ru/C catalyst were found to be with high alloying extent, small average size and low relative crystallinity when the Pt-Ru/C catalyst was prepared with the general chemical reduction method in the mixture solution of tetrahydrofuran (THF) and H2O.
与在纯水中制得的Pt-Ru/C催化剂相比,其Pt-Ru粒子的合金化程度高、平均粒径较小且相对结晶度低,因此,该催化剂对甲醇氧化的电催化活性远高于在纯水中制得的Pt-Ru/C催化剂。
2) homogenization degree
合金均匀化程度
3) alloying schedule
合金化制度
4) galvanneal temperature
合金化温度
1.
This paper studies the effects of galvannealing time and galvanneal temperature on the powdering-resistance of high strength IF galvanized sheet.
选取高强度IF钢热镀锌板,通过控制合金化工艺参数获得了不同w(Fe)和相结构的镀层,研究了合金化时间与合金化温度对于合金化镀层抗粉化性能的影响。