2) HSn70-1A alloy
![点击朗读](/dictall/images/read.gif)
HSn70-1A合金
3) HSn70-1CB alloy
![点击朗读](/dictall/images/read.gif)
HSn70-1CB合金
4) HSn70-1A copper-alloy
![点击朗读](/dictall/images/read.gif)
HSn70-1A铜合金
1.
Synergistic effect of HEDP,ATMP and TTA on corrosion inhibition of HSn70-1A copper-alloy in the industrial recirculation cooling water inoculated with SRB was studied by means of weight loss method、electrochemical polarization and electrochemical impedance spectroscopy(EIS) techniques.
通过静态失重法、极化曲线法、电化学阻抗谱测定了HEDP-ATMP-TTA复配缓蚀剂在循环冷却水介质中硫酸盐还原菌(SRB)作用下对HSn70-1A铜合金的协同缓蚀作用,讨论了缓蚀剂浓度和SRB对铜合金腐蚀行为的影响。
5) HSn70-1 copper tube
![点击朗读](/dictall/images/read.gif)
HSn70-1铜管
6) HSn70-1 round tube
![点击朗读](/dictall/images/read.gif)
HSn70-1圆管