Lower solution treatment temperature of the raw material made the carbide didn't dissolve completely and distributed along the grain boundary like network,so poor chrome happened near the grain boundary and intercrystalline corrosion is produced.
通过对失效件0Cr18Ni9不锈钢制连接螺栓进行失效分析,得出其断裂原因为原材料固溶处理温度偏低,碳化物未充分溶解,并沿晶界呈网状分布,造成晶界附近贫铬,产生晶间腐蚀。
2.
Lower solution treatment temperature of the raw material made the carbide didn t dissolve completely and distributed along the grain boundary like network,so poor chrome happened near the grain boundary and intercrystalline corrosion is produced.
通过对失效件0Cr18Ni9不锈钢制连接螺栓进行失效分析,得出其断裂原因为原材料固溶处理温度偏低, 碳化物未充分溶解,并沿晶界呈网状分布,造成晶界附近贫铬,产生晶间腐蚀。
2)  chromium depletion
贫铬
1.
The chromium depletion at a low-energy boundary segment introduced by twin emission into a random boundary was smaller than that of the original random boundary.
在大角度晶界上形成的局部的低能晶界的贫铬程度明显低于原来的大角度晶界的贫铬程度。
2.
The results showed that nitrogen alloying high purity steels exhibited no chromium depletion at grain boundaries after sensitized heat treatment, and showed mainly general corrosion in boiling 65% HNO 3 solution.
20%)基本上消除敏化态晶间腐蚀,敏化处理不会引起晶界贫铬;当氮含量不超过0。
3)  Cr-depleted layer
贫铬层
4)  poor chrome ore
贫铬矿
1.
Matching poor chrome ore of Xinjiang, Gansu, Qinghai and Vietnam with Indian chrome ore powder, of which Cr2O3 content is between 41%-43% Cr/Fe is 2.
用国内新疆、青海、甘肃等省生产的贫铬矿和越南贫铬矿,配以印度铬矿粉、入炉料控制Cr2O3 41%- 43%,Cr/Fe2。
5)  poor Cr theory
贫铬理论
6)  poor chrome iron ore
贫铬铁矿
补充资料:贫女宝藏
【贫女宝藏】
 (譬喻)一切之凡夫具佛性,譬之贫女之有宝藏也。涅槃经七曰:“我者即是如来藏义。一切众生悉有佛性,即是我义。如是我义从本已来常为无量烦恼所覆,是故众生不能得见。善男子!如贫女人舍内多有真金之藏,家人大小无有知者。时有异人,善知方便语贫女人:我今雇汝,汝可为我芸除草秽。女即答言:我不能也,汝若能示我子金藏然后当速为汝作。(中略)是人即于其家掘出真金之藏。女人见已,心生欢喜,生奇特想,宗仰是人。”同三十四曰:“我又说众生佛性,犹如贫女宅中宝藏,力士额上金刚宝珠,转轮圣王甘露之泉。”
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条