1) zinc-yttrium co-diffusing layer
锌钇共渗层
1.
The microstructure,microhardness and corrosion resistance of the zinc-yttrium co-diffusing layer were investigated by OM,SEM,EDS,XRD,microhardness test and electrochemical corrosion polarization curves test.
7mm的合金反应渗层,渗层由金属间化合物Mg7Zn3、α-Mg饱和固溶体、α-Mg和I-Phase(Mg40Zn55Y5或Mg30Zn60Y10)片层共晶组织构成;该锌钇共渗层的显微硬度有很大的提高,并明显改善了纯镁在5%NaCl溶液中的耐腐蚀性能。
2) zinc-aluminized
锌铝共渗
1.
For improving the corrosion resistance of fixing bolts outer of active amphibian armored cars in the o-ceanic environment, solid zinc-aluminized formula and technology were studied, including the structure, electrochemical performance.
为了适应海洋环境中使用的现役两栖装甲车辆车外固定螺栓防腐蚀性能的要求,除研究了固体锌铝共渗的配方和共渗工艺外,还研究了共渗层的结构、组织和电化学性能。
3) zinc coat
渗锌层
4) penetrating layer
共渗层
1.
By means of the X ray spectrometer and ion probe the micro distribution of rare earth elements in a Re N C penetrating layer is analysed.
用X射线能谱仪及离子探针对Re-N-C共渗层中稀土元素晶粒微观尺度上的分布状况进行了分析。
5) zinc alloyed coating
热扩散渗锌膜层
6) hypereutectic coating
过共晶渗层
补充资料:铝-锌系铸造铝合金
分子式:
CAS号:
性质:以锌为主要合金元素的铸造铝合金,是最早获得工业应用的铝合金之一。在工业中应用的Al-Zn系铸造铝合金成分是5%~14%Zn,2%~3%Cu,6%~8% Si,0.1%~0.7%Mg,并含有少量其他元素。Al-Zn-Cu合金强度较高、切削加工性能和焊接性能良好,但铸造性能和抗腐蚀性能差。Al-Zn-Mg合金具有良好的力学性能和抗腐蚀性能,可以在淬火时效状态下使用,具有更高的强度。另外该合金的熔化温度较高,但其铸造工艺性能较差。Al-Zn-Si合金具有较高的力学性能和良好的铸造性能,广泛用于砂型、金属型和压力铸造。
CAS号:
性质:以锌为主要合金元素的铸造铝合金,是最早获得工业应用的铝合金之一。在工业中应用的Al-Zn系铸造铝合金成分是5%~14%Zn,2%~3%Cu,6%~8% Si,0.1%~0.7%Mg,并含有少量其他元素。Al-Zn-Cu合金强度较高、切削加工性能和焊接性能良好,但铸造性能和抗腐蚀性能差。Al-Zn-Mg合金具有良好的力学性能和抗腐蚀性能,可以在淬火时效状态下使用,具有更高的强度。另外该合金的熔化温度较高,但其铸造工艺性能较差。Al-Zn-Si合金具有较高的力学性能和良好的铸造性能,广泛用于砂型、金属型和压力铸造。