1)  the ball-grinding solid state reaction
室温球磨固相化学反应
1.
The host of fluorescence powder BaMgAl10O17:Eu2+ was prepared by the ball-grinding solid state reaction at room temperature.
采用室温球磨固相化学反应法制备蓝色荧光粉BaMgAl10O17:Eu2+的基质材料,借鉴表面扩散原理对蓝粉进行铕元素的掺杂,用活性碳粉还原得到BaMgAl10O17:Eu2+。
2)  solid-solid state synthesis method at room temperature
室温固-固相化学反应法
3)  room temperature solid-state reaction
室温固相化学反应
1.
Surface-modified lead iodide nanorods were synthesized by one-step room temperature solid-state reaction of lead nitrate with potassium iodide in the presence of a nonionic surfactant, polyethyl- ene glycol.
以硝酸铅和碘化钾为原料,在体系中添加表面活性剂聚乙二醇(PEG),采用一步室温固相化学反应制备出聚乙二醇表面修饰的碘化铅纳米棒,利用X射线衍射,红外光谱,透射电子显微镜,扫描电子显微镜,热分析和元素分析等手段对其进行了表征。
4)  solid-solid state synthesis method
室温固-固化学反应法
5)  solid state reaction at room temperature
室温固相反应
1.
MnO 2 was prepared with solid state reaction at room temperature, MnO 2 powder prepared with this method was nanosized and had large surface area(300m 2/g).
由室温固相反应制备 Mn O2 。
6)  solid-state reaction
室温固相反应
1.
The precursors of nanoparticles were synthesized via microemulsion technique and a solid-state reaction method, respectively.
采用微乳技术、室温固相反应方法制备了纳米颗粒前驱体;选取合适的熔盐介质,对其进行热处理,通过纳米颗粒固相生长制备了氧化物纳米棒、纳米线(晶须)、纳米带和纳米管等一维纳米材料。