1.
Through adjusting its main process parameters,such as entrance temperature,rolling speed,reduction rate and lubrication,using high speed steel rolls and keeping excellent roll surface,the hot rolling sticking could be improved obviously and the roll marks could be avoided.
通过适当调整入口温度、轧制速度、压下率、润滑工艺等主要工艺参数,采用高速钢轧辊并保持良好的辊面质量,可显著改善热轧黏结,从而避免表面辊痕。