1) microoxide
微量组分氧化物
1.
This pexperiment studied the influences of microoxide on the burnability of high calcium cement,added 2% oxide as Li2O,CuO,TiO2 ,etc repectively to the high calcium meal which mineral component is w(C3S)=75%,w(C3A)=7%,w(C4AF)=18% and fired them at 103000℃ and 104000℃,and tested the f-CaO.
在高钙生料[潜在熟料矿物w(C3S)=75%,w(C3A)=7%,w(C4AF)=18%]中,分别掺入2%的Li2O、CuO、TiO2等13种微量组分氧化物,在103000℃和104000℃下煅烧,通过测熟料的f-CaO,研究了外掺各种氧化物对高钙生料易烧性的影响规律。
2) Rare Earth Oxide Component Content
稀土氧化物组分含量
3) oxide component
氧化物组分
5) trace component
微量组分
1.
Determination of eleven trace components in iron oxide powder by inductively coupled plasma atomic emission spectrometry;
电感耦合等离子体原子发射光谱法测定氧化铁粉中11种微量组分
6) trace components
微量组分
1.
The separation of trace components in rare solution is a popular task in the field of separation process.
稀溶液中微量组分的分离是近年来分离过程这一领域的热门课题 ,讨论了超临界萃取 ,膜分离以及泡沫分离技术在这方面的应用及分离方法的选择。
2.
In this paper, we studied the effect of adding trace components in feed on the pervaporation characteristics of chitosan membrane.
本文探讨了在料液中加入微量组分对壳聚糖膜渗透汽化性能的影响。
补充资料:稀土氟氧化物
分子式:
CAS号:
性质:不溶于水,在空气中稳定。有混合稀土氟氧化物也有单一稀土氟氧化物。它们都为斜方或立方结构。可用稀土氧化物与无水氟化氢或氟化物在800~900℃反应而制得。可制取抛光粉。
CAS号:
性质:不溶于水,在空气中稳定。有混合稀土氟氧化物也有单一稀土氟氧化物。它们都为斜方或立方结构。可用稀土氧化物与无水氟化氢或氟化物在800~900℃反应而制得。可制取抛光粉。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条