The semi-solid slurry of ZL101-Sc alloy was manufactured by low superheat pouring,and the effect of Sc on morphology of primary α-Al in ZL101 alloy was researched.
利用低过热度浇注工艺制备了ZL101-Sc铝合金半固态浆料,研究了Sc对半固态合金初生α-Al形貌的影响。
2) Primary α-Al Phase
初生α-Al相
3) primary α phase
初生α相
1.
Rheological behavior of semisolid A356 alloy with different morphology of primary α phases;
液固温区不同初生α相形态A356合金的流变行为
2.
The crack propagation behavior of primary α phase under tension and cyclic load has been observed in-situ by SEM for near-α type TA15 titanium alloy.
利用带载荷台的扫描电镜原位观察了近α型钛合金TA15中初生α相在单向拉伸和循环交变载荷下裂纹的扩展行为 ,结果表明 :单向拉伸时 ,由于初生α相强度高于基体 β转变组织 ,裂纹遇到初生α相时一般不能穿过而是绕过 ;而在交变载荷下 ,由于基体 β转变组织产生循环硬化 ,其强度水平与初生α相相当 ,裂纹遇到初生α相时可直接贯穿 ,并沿与应力垂直的水平方向扩展。
3.
It is shown that the cause resulting in the machining abnormality is coarse strip-shaped primary α phase.
针对钛合金TC4封装壳体加工异常的现象,从壳体的加工工艺过程、钛合金热轧板材化学成分、金相组织等方面进行了详细分析,判定壳体加工异常的原因在于材料中呈粗大长条状分布的初生α相,并分析了钛合金热轧板材中产生粗大长条状初生α相的原因。