1) binder-aggregate ratio
胶砂比
1.
The influences of alkali equivalen(tcount as Na2O),water-binder ratio and binder-aggregate ratio on the carbonation of alkali-activat-ed slag cement mortar were studied.
研究了碱当量(以氧化钠当量计)、水胶比和胶砂比对碱矿渣水泥砂浆抗碳化性能的影响,并与硅酸盐水泥砂浆进行了对比试验。
2) sand-binder ratio
砂胶比
1.
Effect of sand-binder ratio on properties of carbon fiber reinforced mortar;
砂胶比对碳纤维增强水泥砂浆力学性能的影响
2.
The influences of sand-binder ratio, different binders proportion, and different maintain measures on sample strength are studied.
无论采用何种养护方式,石膏样的强度与砂胶比呈双曲线关系,而混合样的强度变化规律则呈抛物线变化。
3) strength ratio of mortar
胶砂强度比
1.
For the same pozzolanic material, the varying trend of K a is similar to that of strength ratio of mortar as fineness was varied.
结果表明 ,Ka 与标准胶砂强度比具有较好的相关关系 。
4) binder-sand mass ratio
胶砂质量比
5) mortar fluidity ratio
胶砂流动度比
1.
The mortar fluidity ratio and th e activity index of mortar at age of 7d ays and 28days were tested.
将不同颗粒群分布的矿渣、水泥按50%比例混合,测其胶砂流动度比和7d、28d抗折、抗压活性指数,应用Origin软件,以宏观性能指标为Z轴,水泥与矿渣D50差为X轴,水泥与矿渣混合样的粉体D50为Y轴,进行三维区域图分析。
6) ratio of water dosage
胶砂需水量比
补充资料:夹布喷砂胶管
分子式:
CAS号:
性质:夹布胶管的一种。产品结构、制造工艺与普通夹布胶管相同。内胶层具有良好的耐磨性能,工作压力为0.6MPa以下,管内径为ф13~76mm。用于常温下以风压输送石英砂、铁砂等,作喷砂除锈及金属表面清扫、打毛之用。
CAS号:
性质:夹布胶管的一种。产品结构、制造工艺与普通夹布胶管相同。内胶层具有良好的耐磨性能,工作压力为0.6MPa以下,管内径为ф13~76mm。用于常温下以风压输送石英砂、铁砂等,作喷砂除锈及金属表面清扫、打毛之用。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条