1) Nd∶KGW crystal
Nd∶KGW晶体
1.
The temperature fields distribution in Nd∶KGW crystal and end-face deformation were obtained by heat exchange equation.
求解热传导方程得出了Nd∶KGW晶体的温度分布和端面形变,进而计算出了热焦距随泵浦功率的变化曲线,并通过实验对其正确性进行了验证。
2) neodymium doped potassium gadolinium tungstate (Nd:KGW) crystal
掺钕钨酸钾钆(KGW)晶体
3) KGW:Nd crystal
Nd晶体
4) Nd∶YVO4 crystal
Nd∶YVO4晶体
1.
With the aim to solve the thermal effect problem of thermal conductive anisotropic laser media end-pumped by LD, a thermal model of Nd∶YVO4 crystal with adiabatic end faces and a cooling circumference was established.
为了解决LD端面泵浦热传导各向异性激光介质产生的热效应问题,建立了端面绝热、侧面冷却的Nd∶YVO4晶体热模型。
5) Nd∶YAG crystal
Nd∶YAG晶体
6) Nd∶GdVO4 crystal
Nd∶GdVO4晶体
1.
The laser consisted of two 808 nm LDs as the pump sources,two Nd∶GdVO4 crystal as laser gain mediums,an AO Q-switch as intracavity modulator and a symmetrical twin-crystal plane-parallel cavity.
采用两台大功率光纤输出半导体激光器端面泵浦两块Nd∶GdVO4晶体,以声光Q开关作为腔内调制元件,用对称结构双晶体串接平行平面谐振腔。
补充资料:[3-(aminosulfonyl)-4-chloro-N-(2.3-dihydro-2-methyl-1H-indol-1-yl)benzamide]
分子式:C16H16ClN3O3S
分子量:365.5
CAS号:26807-65-8
性质:暂无
制备方法:暂无
用途:用于轻、中度原发性高血压。
分子量:365.5
CAS号:26807-65-8
性质:暂无
制备方法:暂无
用途:用于轻、中度原发性高血压。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条