说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
|
|
1) three unequal straight cracks
三裂纹
2) three-dimensional crack
三维裂纹
1.
This model enables rapid approximate computation of the crack surface displacement and the crack front plastic zone size in the three-dimensional crack.
在应用片条合成法计算三维裂纹尖端应力强度因子基础上,推导了在小范围屈服情况下考虑塑性区影响时三维裂纹尖端应力强度因子的求解公式,讨论了塑性区大小对裂尖应力强度因子的影响,其中重点考虑了塑性区对裂纹发展的阻止效应。
2.
Using the Green’s functions,the extended general displacement solutions of three-dimensional crack problem in electro-magneto-thermo-elastic multiphase composites under extended loads are analyzed by boundary element method.
应用位移基本解,磁电热弹材料三维裂纹问题被转化为求解一组以裂纹表面位移间断为未知函数的超奇异积分方程问题。
3) Three dimensional crack
三维裂纹
4) 3-D crack
三维裂纹
1.
3-D cracked J-integral formulas was transformed and treated by coordinate transformations,finite element and Gauss integral.
将三维裂纹J积分进行了坐标变换、有限元及高斯积分处理,并借助于Visual Basic 6。
2.
3-D crack of a compact tension(CT) specimen with concrete size is also analyzed.
通过采用20节点solid186退化奇异单元,利用ANSYS软件,对三维断裂参量进行计算和分析,结果表明位移法和J积分法确定应力强度因子是可行的;对一定尺寸的紧凑拉伸试样三维裂纹进行分析,得出30Cr1Mo1V转子钢裂纹尖端KI随裂纹长度和载荷水平改变时的变化规律,为研究汽轮机转子裂纹扩展规律提供了合理、有效的方法。
5) 3D crack
三维裂纹
1.
We discuss the 3D cracks around cold-expanded holes and simulate their interference prestress release using the engineering software of ANSYS to study the effect of the interference prestress release on stress intensity factors(SIFs) at crack tips.
以冷挤压孔三维裂纹为讨论对象,应用ANSYS大型工程有限元计算软件,在线弹性条件下,模拟由于干涉产生的预应力释放的真实过程,研究预应力释放对裂纹尖端应力强度因子的影响规律。
2.
A series of uniaxial compressive tests on the frozen PMMA with pre-existing 3D cracks were performed in laboratory to investigate the mechanisms of crack propagation and coalescence in brittle materials.
研究结果表明,三维裂纹间的相互作用对裂纹萌生和扩展主要有两种影响,即相互促进或彼此抑制,裂纹演化过程中其空间位置起主要作用。
3.
Modeling of 3D cracks in the specified block has been done with ANSYS.
利用ANSYS有限元计算软件,对材料的三维裂纹进行建模,利用ANSYS自带的应力强度因子的计算功能,对裂纹尖端的应力强度因子进行计算,实现一种对三位裂纹建模和计算其尖端应力强度应子的新思路。
6) triangular area crack
三角区裂纹
1.
This paper studies the formation mechanism of triangular area cracks on continuous cast slabs, analyzes the effects of secondary cooling, steel grades and chemical composition, continuous casting caster circumstance, process and operation, puts forward the measures to prevent triangular area cracks.
研究了连铸板坯三角区裂纹的形成机理,分析了二次冷却、钢种化学成分、铸机状况、工艺操作等因素的影、晌,提出防止三角区裂纹产生的措施。
2.
The type and formation of the triangular area cracks of the continuous casting slab were analyzed though macro examination and scanning the cracks by SEM.
通过对铸坯的低倍检验和三角区裂纹部位的电镜扫描,分析了连铸板坯三角区裂纹的类型和成因;提出了从钢水成分、二冷配水、驱动压力、轻压下、支撑段等方面的改进措施。
3.
According to the current status of triangular area cracks occurring on continuously cast slabs at Nanjing Iron & Steel Co.
针对南钢连铸板坯出现三角区裂纹的现状,通过低倍和硫印结果得出三角区裂纹的具体位置和类型,根据南钢当前的二冷配水情况,分析三角区裂纹产生的原因并提出二冷制度的改进方案。
补充资料:淬火裂纹和非淬火裂纹的特征及实例分析
淬火裂纹是指在淬火过程中或在淬火后的室温放置过程中产生的裂纹。后者又叫时效裂纹。造成淬火开裂的原因很多,在分析淬火裂纹时,应根据裂纹特征加以区分。 一、淬火裂纹的特征 在淬火过程中,当淬火产生的巨大应力大于材料本身的强度时,便会导致裂纹产生。淬火裂纹往往是在马氏体转变开始进行后不久产生的,裂纹的分布则没有一定的规律,但一般容易在工件的棱角槽口、截面突变处形成。 在显微镜下观察到的淬火开裂,可能是沿晶开裂,也可能是穿晶开裂;有的呈放射状,也有的呈单独线条状或呈网状。 因在马氏体转变区的冷却过快而引起的淬火裂纹,往往是穿晶分布,而且裂纹较直,周围没有分枝的小裂纹。 因淬火加热温度过高而引起的淬火裂纹,都是沿晶分布,裂纹尾端尖细,并呈现过热特征:结构钢中可观察到粗针状马氏体;工具钢中可观察到共晶或角状碳化物。 表面脱碳的高碳钢工件,淬火后容易形成网状裂纹。这是因为,表面脱碳层在淬火冷却时的体积胀大比未脱碳的心部小,表面材料受心部膨胀的作用而被拉裂呈网状。 二、非淬火裂纹的特征 淬火后发生的裂纹,不一定都是淬火所造成的,一般可根据下面的特征来区分。 淬火后发现的裂纹,如果裂纹两侧有氧化脱碳现象,则可以肯定裂纹在淬火之前就已经存在。淬火冷却过程中,只有当马氏体转变量达到一定数量时,裂纹才有可能形成。与此相对应的温度,大约在250℃以下。在这样的低温下,即使产生了裂纹,裂纹两侧也不会发生脱碳和出现明显氧化。所以,有氧化脱碳现象的裂纹是非淬火裂纹。 如果裂纹在淬火前已经存在,又不与表面相通,这样的内部裂纹虽不会产生氧化脱碳,但裂纹的线条显得柔软,尾端圆秃,也容易与淬火裂纹的线条刚健有力,尾端尖细的特征区别开来。 三、实例分析 实例一: 40Cr钢制成的转子轴,经锻造、淬火后发现裂纹。裂纹两侧有氧化迹象,经金相检验,裂纹两侧存在脱碳层,而且裂纹两侧的铁素体呈较大的柱状晶粒,其晶界与裂纹大致垂直。结论:裂纹是在锻造时形成的非淬火裂纹。 当工件在锻造过程中形成裂纹时,淬火加热即引起裂纹两侧氧化脱碳。随着脱碳过程的进行,裂纹两侧的碳含量降低,铁索体晶粒开始生核。当沿裂纹两侧生核的铁素体晶粒长大到彼此接触后,便向离裂纹两侧较远的基体方向生长。由于裂纹两侧在脱碳过程中碳浓度的下降,也是由裂纹的开口部位向内部发展,因而为铁素体晶粒的不断长大提供了条件,故最终长大为晶界与裂纹相垂直的柱状晶体。