说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 纳米碳化钒
1)  nano-sized vanadium carbide
纳米碳化钒
1.
The nano-sized vanadium carbide(V8C7) is prepared by solution-derived precursor method with ammonium vanadate(NH4VO3) and nanometer carbon black as raw material.
以偏钒酸铵和纳米炭黑为原料,采用水溶液前驱体方法制备纳米碳化钒(V8C7)粉末。
2)  vanadium nitride nanopowder
纳米氮化钒
3)  vanadium oxide nanopowders
氧化钒纳米粉
4)  Vanadium oxide nanotubes
钒氧化物纳米管
1.
Vanadium oxide nanotubes (VO x-NTs) were synthesized in a rheological phase reaction followed by self-assembling process and characterized by XRD, SEM, TEM, Raman, ESR, TG-DTA, XPS, and simulated battery.
采用流变相 -纳米自组装新方法合成了钒氧化物纳米管 ( VOx-NTs) ,并通过 XRD,SEM,TEM,Raman,ESR,TG-DTA,XPS及模拟电池等技术手段对产物的结构和性能进行了表征和测试 。
2.
Vanadium oxide nanotubes(VONTs) represent the redox activity due to their mixedoxidation state and their unique electron transported character attribute to the anisotropicstructures.
钒氧化物纳米管(VONTs)的混合价态使其具有氧化活性,而它的各向异性结构又使其具有独特的电输运特性,同时纳米管层间的协同离子交换行为也使得其有可能在层间嵌入大量的功能阴、阳离子。
5)  nano vanadium oxide
纳米钒氧化物
6)  nanovanadium oxide thin film
纳米氧化钒薄膜
补充资料:硅-氧化钠-五氧化二钒系湿敏材料
分子式:
CAS号:

性质:一种感湿体材料。主晶相为硅粉,氧化钠和五氧化二钒起助熔体和黏结作用。680℃固相烧结法制取。游离硅粒保证瓷体的低电阻率,氧化钠和五氧化二钒有利于吸收水分,受潮后使硅粒之间的电阻值显著下降。材料响应速度慢,吸湿时间≥5min,脱湿时间≥l0min,宜用于中湿和湿度变化不太快的场合。制作的湿敏元件体积小、机械强度好、阻值范围可调,工作寿命长。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条