1)  Micro-powder mixture of steel slag and granulated blast furnace slag
钢渣矿渣微粉
2)  super-fine steel slag powder
钢渣矿粉
3)  steel-slag powder
钢渣微粉
1.
Utilization of steel-slag powder is a new technology, which represents the top level of the research on steel slag resources currently.
钢渣微粉的利用代表目前钢渣资源化利用的最高水平。
4)  steel slag powder
钢渣微粉
1.
The effect of steel slag powder on road properties and freezing and thawing resistance of concrete was studied.
研究了钢渣微粉对混凝土路用性能和抗冻融循环能力的影响。
2.
Properties of concrete with parts of cement replaced by steel slag powder, including compressive strength, Cl~- permeability, carbonation, gas permeability and drying shrinkage were investigated.
试验研究了钢渣微粉对混凝土抗压强度、干缩、碳化、抗氯离子渗透、气渗等性能指标的影响。
3.
The chemical components,phase components,and micro-structure properties of steel slag powder are analyzed.
首先选用多种分析方法对钢渣微粉的化学成分、相成分和微观形貌等进行分析;然后在沥青混合料中掺加钢渣微粉,研究用钢渣微粉部分或全部替代矿粉对沥青混合料性能的影响。
5)  slag micropowder
矿渣微粉
1.
Experimental study on compound admixture of slag micropowder
矿渣微粉基复合掺合料的试验研究
2.
A research is made on the effect of slag micropowder used as admixture on the performance of cement by adding different proportion of slag micropowder to the P·Ⅰ52.
5水泥中掺入不同比例的矿渣微粉,研究了矿渣微粉作混合材对水泥性能的影响。
3.
Taking volume decrement of blast furnace slag (BFS) and fly ash pump concrete in plastic stage as quantification basis for evaluation of pump concrete plastic shrinkage proves that plastic shrinkage crack of pump concrete has certain internal relation with adding slag micropowder.
以掺矿粉粉煤灰泵送混凝土塑性阶段的体积减缩量作为评价泵送混凝土塑性收缩的量化依据,证实了掺用矿渣微粉与混凝土塑性收缩裂缝有一定的内在关系,尤其是夏季采用25%以上的大掺量用于现浇楼板等薄壁结构混凝土工程,极易引发混凝土塑性裂缝。
6)  ground granulated blast furnace slag
矿渣微粉
1.
In the paper,the effects of sulfate and magnesium salt erosion on ordinary cement mortar samples and high performance concrete cement mortar samples with ground granulated blast furnace slag soaked in 4 density sulfate and magnesium salt solutions are studied.
结合工程实际,以在4种不同浓度的SO2-4,Mg2+侵蚀溶液中浸泡的普通水泥胶砂试件和掺矿渣微粉高性能混凝土胶砂试件为对比试件进行研究,通过测定和观察试件在浸泡期为28d、2个月、4个月、6个月、8个月、10个月、12个月的强度损失和形态形貌变化,用抗折强度和抗蚀系数来评定其抗侵蚀性能。
2.
Cement concrete adhesiveness and water retention effectiveness have been improvement of different level after incorporating ground granulated blast furnace slag (GGBS).
掺入矿渣微粉后混凝土的粘聚性和保水性都有不同程度的改善;矿渣微粉具有一定的辅助减水作用,随着矿渣粉取代水泥量的增加,混凝土用水量不变时,坍落度呈增加趋势,这一趋势随水胶比的降低和掺量的增加更为显著。
补充资料:活性微粒矿粉
分子式:
CAS号:

性质:以矿物质(和碳酸钙、陶土等)为原料,经粉碎细化和用偶联剂等进行活化处理所得的产品。细度为325目左右,与橡胶具有较强的亲和性,有较显著的补强作用。可以部分代替炭黑在橡胶中使用。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。